Polimeri Europa SINKRAL A22V ABS  (discontinued **)

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Molded
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polimeri Europa SINKRAL A22V ABS  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,095-25-09-25 Very high flow grade for fast cycle injection moulding. Particularly recommended for the domestic appliance industry (vacuum cleaners) and kitchen/bathroom accessories.Unfilled. Suitable for Injection Molding. Supplied as pellets. Contains lubricant and release agent.ISO data. Information provided by EnichemPolimeri Europa now has Enichem's plastics businesses. This grade is no longer in the product line.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
Water Absorption 1.0 %
1.0 %
Moisture Absorption at Equilibrium 0.20 %
0.20 %
Humidity Absorption
Melt Flow 35 g/10 min

@Load 10.0 kg,
Temperature 220 °C
35 g/10 min

@Load 22.0 lb,
Temperature 428 °F
cm³/10 min
Mechanical Properties Metric English Comments
Tensile Strength, Yield 43.0 MPa
6240 psi
50 mm/min
Elongation at Break 10 %
10 %
Nominal
Elongation at Yield 3.1 %
3.1 %
50 mm/min
Tensile Modulus 2.50 GPa
363 ksi
1 mm/min
Charpy Impact Unnotched 11.0 J/cm²
52.4 ft-lb/in²
7.00 J/cm²

@Temperature -30.0 °C
33.3 ft-lb/in²

@Temperature -22.0 °F
Charpy Impact, Notched 0.500 J/cm²

@Temperature -30.0 °C
2.38 ft-lb/in²

@Temperature -22.0 °F
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 90.0 µm/m-°C

@Temperature 20.0 °C
50.0 µin/in-°F

@Temperature 68.0 °F
Deflection Temperature at 0.46 MPa (66 psi) 92.0 °C
198 °F
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C
176 °F
Vicat Softening Point 97.0 °C
207 °F
50°C/hr; 50N
Glass Transition Temp, Tg 107 °C
225 °F
10°C/min test
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
Dielectric Constant 2.9

@Frequency 1e+6 Hz
2.9

@Frequency 1e+6 Hz
3.0

@Frequency 100 Hz
3.0

@Frequency 100 Hz
Dielectric Strength 30.0 kV/mm
762 kV/in
Comparative Tracking Index 600 V
600 V
Users viewing this material also viewed the following: