Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 20.0 J/cm² | 95.2 ft-lb/in² | dry; ISO 179-1/1eU |
Murtfeldt Murytal® H Acetal Homopolymer In addition to the excellent properties of Murytal® C, Murytal® H is stronger and more rigid with a lower expansion coefficient.Special Properties:• High rigidity• Excellent ability to regain it.. |
|||
Charpy Impact Unnotched | >= 20.0 J/cm² | >= 95.2 ft-lb/in² | ISO 179 |
Murtfeldt Murytal® H Acetal Homopolymer In addition to the excellent properties of Murytal® C, Murytal® H is stronger and more rigid with a lower expansion coefficient.Special Properties:• High rigidity• Excellent ability to regain it.. |
|||
Charpy Impact Unnotched | 20.0 J/cm² | 95.2 ft-lb/in² | ISO 179/1eU |
Aardvark Polymers AARTEL® 2000 Rotational Molding Resin Aartel® 2000 POM is a premium homopolymer acetal for rotational molding applications. Aartel® 2000 offers high performance properties and is a high flow, fast cycling polymer.Information prov.. |
|||
Charpy Impact Unnotched | 20.0 J/cm² @Temperature -30.0 °C |
95.2 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Aardvark Polymers AARTEL® 2000 Rotational Molding Resin Aartel® 2000 POM is a premium homopolymer acetal for rotational molding applications. Aartel® 2000 offers high performance properties and is a high flow, fast cycling polymer.Information prov.. |
|||
Charpy Impact Unnotched | 20.0 J/cm² | 95.2 ft-lb/in² | ISO 179/1eU |
DuPont Performance Polymers Delrin® 900P NC010 Acetal (POM)
(Unverified Data**) Low Viscosity Acetal Homopolymer with Improved Processing Delrin 900P is a low viscosity acetal homopolymer for injection molding. It has improved processing thermal stability good mechanical proper.. |
|||
Charpy Impact Unnotched | 20.0 J/cm² @Temperature -30.0 °C |
95.2 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DuPont Performance Polymers Delrin® FG511DP NC010 Acetal (POM)
(Unverified Data**) Nucleated Medium Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG511DP is a medium viscosity acetal homopolymer with improved thermal stability and modifications for mo.. |
|||
Charpy Impact Unnotched | 20.0 J/cm² | 95.2 ft-lb/in² | ISO 179/1eU |
DuPont Performance Polymers Delrin® FG900P NC010 Acetal (POM)
(Unverified Data**) Low Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG900P is a low viscosity acetal homopolymer with improved thermal stability. It has been developed for consideration .. |
|||
Charpy Impact Unnotched | 20.0 J/cm² | 95.2 ft-lb/in² | |
BASF Novolen® 3240 NC Polypropylene Grade containing nucleating agent for transparent injection molded parts.Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact Unnotched | 20.0 J/cm² @Temperature -30.0 °C |
95.2 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
BASF Ultraform H 2320 006 Q600 POM Ultraform H2320 006 is a high-molecular-weight grade of POM for injection molding. It conforms to FDA requirements of 21 CFR 177.2470. |
|||
Charpy Impact Unnotched | 20.0 J/cm² | 95.2 ft-lb/in² | ISO 179 |
BASF Ultraform N 2310P Q600 POM Ultraform N2310P Q600 is a general-purpose injection molding POM grade containing special lubricant. Low frictional coefficient giving extremely low wear with otherwise unaltered mechanical propert.. |
|||
Charpy Impact Unnotched | 20.0 J/cm² | 95.2 ft-lb/in² | ISO 179 |
BASF Ultraform N 2320 U03 UNC Q600 POM Ultraform N2320 U03 UNC Q600 is a rapidly freezing UV stabilized general-purpose injection molding grade. |
|||
Charpy Impact Unnotched | 20.0 J/cm² | 95.2 ft-lb/in² | |
BASF Novolen® 2240 P Polypropylene Nucleated grade for injection moldings.Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact Unnotched | 20.0 J/cm² | 95.2 ft-lb/in² | |
BASF Novolen® 3248 RC Polypropylene Grade containing nucleating and antistatic agents for injection molded parts.Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact Unnotched | 20.0 J/cm² @Temperature -30.0 °C |
95.2 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
BASF Ultramid® B3S BK00464 PA6 (Dry) Ultramid B3S BK00464 is an easy flowing, pigmented black, finely crystalline injection molding PA6 grade. It conforms to FDA requirements of 21 CFR 177.1500. |