Polymer Property : Izod Impact, Unnotched = 0.374 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 0.374 J/cm

@Thickness 3.17 mm
0.700 ft-lb/in

@Thickness 0.125 in
ASTM D256
Niche Polymer PA66GM40BK Nylon 66, 40% Mineral Fiber Filled
Information provided by Niche Polymer
Izod Impact, Unnotched 0.374 J/cm

@Thickness 3.17 mm
0.700 ft-lb/in

@Thickness 0.125 in
ASTM D256
Niche Polymer PA66GM40N Nylon 66, 40% Mineral Fiber Filled
Information provided by Niche Polymer
Izod Impact, Unnotched 0.374 J/cm

@Thickness 3.17 mm
0.700 ft-lb/in

@Thickness 0.125 in
ASTM D256
Niche Polymer PA6GM40BK Nylon 6, 40% Mineral Fiber Filled
Information provided by Niche Polymer
Izod Impact, Unnotched 0.374 - 16.4 J/cm
0.700 - 30.7 ft-lb/in
Average value: 5.72 J/cm Grade Count:9
Overview of materials for Nylon 6, 40% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Mineral Filled". Each property range of values reported is minimum and maximum values of ap..
Izod Impact, Unnotched 0.374 - 7.47 J/cm
0.700 - 14.0 ft-lb/in
Average value: 3.28 J/cm Grade Count:13
Overview of materials for Nylon 66, 40% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Mineral Filled". Specific grades with primary filler content between 35% and 44% are inclu..
Izod Impact, Unnotched 0.374 J/cm

@Temperature -40.0 °C
0.700 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Spartech 513 Static Dissipative Control Sheet
Description: Static Control SheetInformation provided by Spartech.
Izod Impact, Unnotched 0.374 J/cm

@Temperature -40.0 °C
0.700 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Spartech 617 Static Dissipative Control Sheet
Description: Static Control SheetInformation provided by Spartech.
Izod Impact, Unnotched 0.374 J/cm

@Temperature -40.0 °C
0.700 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Spartech 829 Static Conductive Control Sheet
Description: Static Control SheetInformation provided by Spartech.
Izod Impact, Unnotched 0.374 J/cm

@Temperature -40.0 °C
0.700 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Spartech Spectar® Copolyester Sheet
Description: Copolyester SheetSpectar is a registered trademark of Eastman Chemical Company.Information provided by Spartech.
Izod Impact, Unnotched 0.374 J/cm

@Temperature -40.0 °C
0.700 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Spartech Sta-Tuf High Impact Thermoplastic Alloy Sign Grade Sheet
Description: Sign Grade SheetInformation provided by Spartech.
Izod Impact, Unnotched 0.374 J/cm

@Temperature -40.0 °C
0.700 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Spartech Spectar® UV Copolyester Sheet
Description: Copolyester SheetSpectar is a registered trademark of Eastman Chemical Company.Information provided by Spartech.