Material Notes:
Available in North America Features: Food Contact Acceptable and High DensityAgency Ratings: FDA 21 CFR 177.1520RoHS Compliant Form: Pellets Information provided by Entec
Physical Properties Metric English Comments
Specific Gravity 0.953 g/cc
0.953 g/cc
ASTM D792
Melt Flow 6.6 g/10 min

@Load 2.16 kg,
Temperature 190 °C
6.6 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 22.4 MPa
3250 psi
ASTM D638
Tensile Strength, Yield 28.3 MPa
4110 psi
ASTM D638
Elongation at Break 7.3 %
7.3 %
ASTM D638
Flexural Modulus 1.25 GPa
181 ksi
ASTM D790
Thermal Properties Metric English Comments
Vicat Softening Point 127 °C
261 °F
Rate A (50°C/h), Loading 1 (10 N); ASTM D1525