Multibase TPSiV™ 3340-55A Thermoplastic Silicone Vulcanizate

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Vulcanizate Elastomer (TPV) , Polyurethane, TP , Silicone, Thermoplastic
Manufacturer Multibase
Trade Name TPSiV™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase TPSiV™ 3340-55A Thermoplastic Silicone Vulcanizate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
These materials are a novel family of TPV products based on cross-linked silicone rubber dispersed into various engineering thermoplastics. The dispersion of the silicone internal phase is produced by dynamic “vulcanization” or cross-linking of silicone polymers within the thermoplastic organic phase and results in a stable droplet type morphology as shown in the TEM micrograph. TPSiV™ combines the elastomeric performance of silicone rubber with the melt re-processability and thermal and chemical resistance of engineering thermoplastics.Thermoplastic polyurethane based TPSiV™ (3010, 3011, 3111, 3040, 3340 grades) combine the benefits of excellent abrasion resistance from the polyurethane as well as the lower coefficient of friction and improved temperature properties from the silicone rubber.TPSiV™ 3340-55A / 60A / 65A: Designed for excellent UV stability in all colors and is used in injection molding applications, specifically overmolding and co-molding on PC and ABS. They are commonly used in communication devices, computers, and electronic devices.Information provided by Multibase, a Dow Corning Company
Physical Properties Metric English Comments
Specific Gravity 1.15 g/cc
1.15 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 55
55
10 sec; ASTM D2240
Tensile Strength at Break 3.00 MPa
435 psi
ASTM D412
Elongation at Break 400 %
400 %
ASTM D412
Tear Strength 15.1 kN/m
86.2 pli
ASTM D412
Thermal Properties Metric English Comments
Flammability, UL94 HB
HB
Processing Properties Metric English Comments
Rear Barrel Temperature 170 °C
338 °F
Middle Barrel Temperature 180 °C
356 °F
Front Barrel Temperature 190 °C
374 °F
Nozzle Temperature 195 °C
383 °F
Mold Temperature 10.0 - 30.0 °C
50.0 - 86.0 °F
Drying Temperature 80.0 °C
176 °F
Dry Time 2 - 4 hour
2 - 4 hour
Descriptive Properties Value Comments
Injection Rate Moderate-Fast