Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 6.00 J/cm² @Temperature -20.0 °C |
28.6 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom PLASTAMID® 66 BT N 27 B PA66 PA66 for compounding, modified for general use, with excellent manufacturing properties. Use: automotive, engineering, electrical and consumer-goods industry - electrical tools, fasteners, clamps, h.. |
|||
Charpy Impact Unnotched | 6.00 J/cm² @Temperature 23.0 °C |
28.6 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom SLOVALEN PC 52 T 20 Polypropylene Copolymer, 20% Micronized Talc FeaturesModified copolymer PP for injection moulding with the content of 20% micronized, floated, chemically modified talc. General application - packing material, garden flower-pots, toys, furnitu.. |
|||
Charpy Impact Unnotched | 6.00 J/cm² @Temperature 23.0 °C |
28.6 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom SLOVAMID 6 GF 30 LS Polyamide 6, 30% Glass Fiber, UV Stabilization FeaturesPA 6 for injection moulding, chemically reinforced with 30% glass fiber, stabilized against UV-radiation. Used for the grips of electric tools, hobby tools, gears, covers of electric tools... |
|||
Charpy Impact Unnotched | 6.00 J/cm² @Temperature 23.0 °C |
28.6 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
DuPont Performance Polymers Crastin® SK615SF NC010 PBT
(Unverified Data**) Crastin® SK615SF is a 30% glass fiber reinforced, low viscosity polybutylene terephthalate for injection molding. It has high flow characteristics and is specifically suitable for super fast produc.. |
|||
Charpy Impact Unnotched | 6.00 J/cm² @Temperature 23.0 °C |
28.6 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
DSM Akulon® Ultraflow™ K-FKGS6 Nylon 6-30% Glass Reinforced (European and Asian Grade) (Cond)
(discontinued * The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact Unnotched | 6.00 J/cm² @Temperature 23.0 °C |
28.6 ft-lb/in² @Temperature 73.4 °F |
Conditioned; ISO 179/1eU |
Lanxess Durethan® DP 2131/20 H2.0 900051 Nylon 6, 20% Glass Fiber PA 6, injection molding grade, 20% glass fibers, better surface resistance to alcoholic calcium chloride-solution than BKV 20 H2.0, good heat-ageing resistance and weather resistance |
|||
Charpy Impact Unnotched | 6.00 J/cm² @Temperature 23.0 °C |
28.6 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Lanxess Pocan® B 3225 XF 000000 PBT, 20% Glass Fiber PBT, 20% glass fibers, injection molding, improved flowability |
|||
Charpy Impact Unnotched | 6.00 J/cm² @Temperature 23.0 °C |
28.6 ft-lb/in² @Temperature 73.4 °F |
d.a.m.; ISO 179-1eU |
Lanxess Durethan® BKV 30 G W1 901317 Nylon 6, Glass Fiber Reinforced PA 6, 30% glass fibers, injection molding, weather stabilizedInformation provided by LANXESS. |
|||
Charpy Impact Unnotched | 6.00 J/cm² @Temperature -30.0 °C |
28.6 ft-lb/in² @Temperature -22.0 °F |
d.a.m.; ISO 179-1eU |
Lanxess Durethan® BKV 30 H2.0 EF 000000 Nylon 6, Glass Fiber Reinforced PA 6, 30% glass fibers, injection molding, improved flowability, heat-aging stabilizedInformation provided by LANXESS. |
|||
Charpy Impact Unnotched | 6.00 J/cm² @Temperature -30.0 °C |
28.6 ft-lb/in² @Temperature -22.0 °F |
d.a.m.; ISO 179-1eU |
Lanxess Durethan® ECO BV 35 H2 900500 Nylon 6, 35% Glass Fiber PA 6, 35% glass fibers, injection molding, heat-ageing stabilized, contains 30% pre-consumer recycled materialInformation provided by LANXESS. |
|||
Charpy Impact Unnotched | 6.00 J/cm² @Temperature -30.0 °C |
28.6 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Ultem ATX102R PEI+PCE 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region. |
|||
Charpy Impact Unnotched | 6.00 J/cm² @Temperature -20.0 °C |
28.6 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eU |
Borealis Daplen™ EE158AI Polypropylene TPO Compound Daplen™ EE158AI is a 13% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness, give.. |
|||
Charpy Impact Unnotched | 6.00 J/cm² @Temperature 23.0 °C |
28.6 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polyram PlusTek PA840G13 Nylon 66 for Injection Molding, 13% Glass Fiber Reinforced, Impact Modified, Heat Resistant Impact modified, 13% glass fiber reinforced, heat resistant Nylon 66 for injection molding applications.Information provided by Polyram. |
|||
Charpy Impact Unnotched | 6.00 J/cm² @Temperature -20.0 °C |
28.6 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eU |
Borealis Xmod™ GD302HP Polypropylene, Glass Fiber Reinforced Xmod™ GD302HP is a 30 % chemically coupled high performance glass fiber reinforced polypropylene compound intended for injection molding. This material has an excellent balance between impact stre.. |
|||
Charpy Impact Unnotched | 6.00 J/cm² @Temperature -30.0 °C |
28.6 ft-lb/in² @Temperature -22.0 °F |
dry; ISO 179/1eU |
DSM Stanyl® 46HF4530 PA46-GF30 30% Glass Reinforced, Heat Stabilized, High Flow, for E&E applications |
|||
Charpy Impact Unnotched | 6.00 J/cm² @Temperature 23.0 °C |
28.6 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
DSM Stanyl® TE250F6 Nylon 46-30% Glass Reinforced (European and Asian Grade) (Cond) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Charpy Impact Unnotched | 6.00 J/cm² @Temperature 23.0 °C |
28.6 ft-lb/in² @Temperature 73.4 °F |
Edgew 80x10x4 sp=62; ISO 179/1eU |
Eurostar Star X RF003IU2-BK3047 PA66, Glass Fiber Filled, Impact Modified, Injection Molded Star X RF003IU2-BK3047 is an Impact Modified, Glass Fiber Reinforced, UV stabilized Polyamide 66/6 Injection Molding (also known as Star X D 1010 14V/3/047)Information provided by Eurostar. |
|||
Charpy Impact Unnotched | 6.00 J/cm² @Temperature -30.0 °C |
28.6 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DSM Arnite® AV2 370 HF PET-GF35 35% Glass Reinforced, Brake Booster Body Valves, High Flow |
|||
Charpy Impact Unnotched | 6.00 J/cm² @Temperature -30.0 °C |
28.6 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DSM Arnite® AV2 370 XL PET-GF35 35% Glass Reinforced, Low Outgassing |
|||
Charpy Impact Unnotched | 6.00 J/cm² @Temperature 23.0 °C |
28.6 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
DSM Stanyl® TW250F6 Nylon 46-30% Glass Reinforced (European Grade) (Cond) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Charpy Impact Unnotched | 6.00 J/cm² @Temperature -30.0 °C |
28.6 ft-lb/in² @Temperature -22.0 °F |
Edgew 80x10x4 sp=62; ISO 179/1eU |
Eurostar Staramide BG4ST43 PA6, Glass Fiber Filled, Impact Modified, Injection Molded Staramide BG4ST43 is an Impact Modified and Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Charpy Impact Unnotched | 6.00 J/cm² @Temperature -30.0 °C |
28.6 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
BASF Ultramid® KR 4355 G5 25% Glass Filled PA6/6T (Dry) Description: 25% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r.. |
|||
Charpy Impact Unnotched | 6.00 J/cm² @Temperature -30.0 °C |
28.6 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Akro-Plastic Akromid® T6 GF 40 (3500) PPA Dry, 40% Glass Filled The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high.. |
|||
Charpy Impact Unnotched | 6.00 J/cm² @Temperature 23.0 °C |
28.6 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
BASF Ultramid® B35EG3 BK 00564 15% Glass Filled PA6 (Dry) Description: 15% glass-fiber reinforced injection-molding grade for gIT applications such as, for example, steering column switches, vehicle mirror housings and the wheels of mountain bikes.Informat.. |
|||
Charpy Impact Unnotched | 6.00 J/cm² @Temperature 23.0 °C |
28.6 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVALEN PC 91 T 30 PP, 30% mineral filling FeaturesModified copolymer PP for injection moulding with the content of 30% microground, floated, chemically modified talc. General application - packing material, garden flower-pots, toys, furnitu.. |
|||
Charpy Impact Unnotched | 6.00 J/cm² @Temperature 23.0 °C |
28.6 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom SLOVALEN PH 51 T 10 Polypropylene Homopolymer, 10% Mineral Filled FeaturesModified homopolymer PP for injection moulding with the content of 10% mineral filler. Increased rigidity, strength and thermal use up to 120°C. Decreased shrinkage. General application .. |
|||
Charpy Impact Unnotched | 6.00 J/cm² @Temperature 23.0 °C |
28.6 ft-lb/in² @Temperature 73.4 °F |
|
LATI Latamid 66 H2 G/25-V0KB4 PA 66, 25% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with red phosphorous. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaIn.. |
|||
Charpy Impact Unnotched | 6.00 J/cm² @Temperature -30.0 °C |
28.6 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Sax Polymers SAXATEC 4115 Acrylonitrile Styrene Acrylate SAXATEC 4115 is a medium viscosity, weatherable ASA injection molding grade, characterized by high impact strength, high stiffness and good resistance to heat distortion.Information provided by SAX .. |
|||
Charpy Impact Unnotched | 6.00 J/cm² @Temperature 23.0 °C |
28.6 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Lanxess Pocan® DP B 3235 XF 901510 PBT, 30% Glass Fiber