Eurostar Star X RF003IU2-BK3047 PA66, Glass Fiber Filled, Impact Modified, Injection Molded

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Glass Reinforced, Impact Grade
Manufacturer Eurostar Engineering Plastics
Trade Name Star X
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eurostar Star X RF003IU2-BK3047 PA66, Glass Fiber Filled, Impact Modified, Injection Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Star X RF003IU2-BK3047 is an Impact Modified, Glass Fiber Reinforced, UV stabilized Polyamide 66/6 Injection Molding (also known as Star X D 1010 14V/3/047)Information provided by Eurostar.
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
ASTM D792
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm

@Thickness 4.00 mm
0.0050 - 0.0070 in/in

@Thickness 0.157 in
E2P method
Ash 14 %
14 %
ISO 3451
Mechanical Properties Metric English Comments
Tensile Strength, Yield 90.0 MPa
13100 psi
ISO 527
Elongation at Break 4.0 %
4.0 %
ISO 527
Tensile Modulus 4.40 GPa
638 ksi
1 mm/min; ISO 527
Flexural Strength 115 MPa
16700 psi
ISO 178
Flexural Modulus 3.30 GPa
479 ksi
ISO 178
Izod Impact, Notched (ISO) 6.00 kJ/m²

@Temperature -30.0 °C
2.86 ft-lb/in²

@Temperature -22.0 °F
80x10x4; ISO 179/1eA
13.0 kJ/m²

@Temperature 23.0 °C
6.19 ft-lb/in²

@Temperature 73.4 °F
80x10x4; ISO 179/1eA
Izod Impact, Unnotched (ISO) 50.0 kJ/m²

@Temperature 23.0 °C
23.8 ft-lb/in²

@Temperature 73.4 °F
80x10x4; ISO 180/1U
50.0 kJ/m²

@Temperature -30.0 °C
23.8 ft-lb/in²

@Temperature -22.0 °F
80x10x4; ISO 180/1U
Charpy Impact Unnotched 5.50 J/cm²

@Temperature -30.0 °C
26.2 ft-lb/in²

@Temperature -22.0 °F
Edgew 80x10x4 sp=62; ISO 179/1eU
6.00 J/cm²

@Temperature 23.0 °C
28.6 ft-lb/in²

@Temperature 73.4 °F
Edgew 80x10x4 sp=62; ISO 179/1eU
Charpy Impact, Notched 0.600 J/cm²

@Temperature -30.0 °C
2.86 ft-lb/in²

@Temperature -22.0 °F
Edgew 80x10x4 sp=62; ISO 179/1eA
1.15 J/cm²

@Temperature 23.0 °C
5.47 ft-lb/in²

@Temperature 73.4 °F
Edgew 80x10x4 sp=62; ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 215 °C
419 °F
Edgew 120x10x4, sp=100 mm; ISO 75/Ae
Processing Properties Metric English Comments
Zone 1 260 - 280 °C
500 - 536 °F
Zone 2 270 - 280 °C
518 - 536 °F
Zone 3 270 - 290 °C
518 - 554 °F
Melt Temperature 270 - 290 °C
518 - 554 °F
Mold Temperature 60.0 - 90.0 °C
140 - 194 °F
Drying Temperature 75.0 - 85.0 °C

@Time 14400 - 21600 sec
167 - 185 °F

@Time 4.00 - 6.00 hour
Moisture Content 0.20 %
0.20 %