Polymer Property : Izod Impact, Unnotched (ISO) = 21.0 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 21.0 kJ/m²
9.99 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics Lexan® JK500 PC+ABS (Asia Pacific)
10% GR, ECO conforming FR, PC+ABS for thinwall molding applications.
Izod Impact, Unnotched (ISO) 21.0 kJ/m²
9.99 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP FARADEX NX07344 PC+ABS (Asia Pacific)
Faradex NX07344 is a compound based on PC+ABS blend resin containing non-brominated and non-chlorinated flame retardant system, Stainless Steel and glass fiber. Added features of this material incl..
Izod Impact, Unnotched (ISO) 21.0 kJ/m²

@Temperature -30.0 °C
9.99 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP FARADEX NX07344 PC+ABS (Asia Pacific)
Faradex NX07344 is a compound based on PC+ABS blend resin containing non-brominated and non-chlorinated flame retardant system, Stainless Steel and glass fiber. Added features of this material incl..
Izod Impact, Unnotched (ISO) 21.0 kJ/m²
9.99 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP AL003 ABS
LNP LUBRICOMP* AL003 is a compound based on Acrylonitrile Butadiene Styrene resin containing 15% PTFE. Added features of this material include: Internally Lubricated.
Izod Impact, Unnotched (ISO) 21.0 kJ/m²
9.99 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP AL003 ABS (Europe-Africa-Middle East)
LNP LUBRICOMP* AL003 is a compound based on Acrylonitrile Butadiene Styrene resin containing PTFE. Added features of this material include: Internally Lubricated.
Izod Impact, Unnotched (ISO) 21.0 kJ/m² - NB
9.99 ft-lb/in² - NB
Average value: 96.6 kJ/m² Grade Count:64
Overview of materials for Polycarbonate/ABS Alloy, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Unreinforced". Each property range of values reported is minimum and maximum va..
Izod Impact, Unnotched (ISO) 21.0 - 52.0 kJ/m²

@Temperature -40.0 - -30.0 °C
9.99 - 24.7 ft-lb/in²

@Temperature -40.0 - -22.0 °F
Average value: 32.0 kJ/m² Grade Count:7
Overview of materials for Polycarbonate/ABS Alloy, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Glass Fiber Filled". Each property range of values reported is minimum and maxi..
Izod Impact, Unnotched (ISO) 21.0 kJ/m² - NB
9.99 ft-lb/in² - NB
Average value: 24.5 kJ/m² Grade Count:8
Overview of materials for Polypropylene, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Molded". Each property range of values reported is minimum and maximum values of appropri..
Izod Impact, Unnotched (ISO) 21.0 kJ/m²
9.99 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP AL003 ABS (Asia Pacific)
LNP LUBRICOMP* AL003 is a compound based on Acrylonitrile Butadiene Styrene resin containing PTFE. Added features of this material include: Internally Lubricated.
Izod Impact, Unnotched (ISO) 21.0 kJ/m²
9.99 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP STAT-KON Cycoloy_JK800 PC+ABS
LNP* Stat-kon* Cycoloy_JK800 compound is an 8% carbon fiber reinforcedPC+ABS, electrostatic dissipative ECO conforming FR. Good hydrolytic stability.
Izod Impact, Unnotched (ISO) 21.0 kJ/m²
9.99 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP STAT-KON EX11402 PEI
LNP* STAT-KON* EX11402 is a compound based on Polyetherimide resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive.
Izod Impact, Unnotched (ISO) 21.0 kJ/m²
9.99 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP STAT-KON OEL32 PPS - Linear
LNP* STAT-KON* OCL32 is a compound based on PPS - Linear resin containing 10% Carbon Fiber, 15% PTFE. Added features of this grade include: Electrically Conductive, Wear Resistant.
Izod Impact, Unnotched (ISO) 21.0 kJ/m²
9.99 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP AF004L ABS
LNP* THERMOCOMP* AF004L is a compound based on ABS resin containing 20% Glass Fiber. Added feature of this material is: Low Extractible.
Izod Impact, Unnotched (ISO) 21.0 kJ/m²
9.99 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP Lexan_JK500 PC+ABS
LNP* Thermocomp* Lexan_JK500 compound is a 10% GR, ECO conforming FR, PC+ABS for thinwall molding applications.
Izod Impact, Unnotched (ISO) 21.0 kJ/m²
9.99 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP Lexan_JK500 PC+ABS (Asia Pacific)
10% GR, ECO conforming FR, PC+ABS for thinwall molding applications.
Izod Impact, Unnotched (ISO) 21.0 kJ/m²
9.99 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP OF008A PPS (Asia Pacific)
LNP* Thermocomp* OF008A is a compound based on PPS - Branched resin containing Glass Fiber.This product is also known as Thermocomp* OF-1008.
Izod Impact, Unnotched (ISO) 21.0 kJ/m²
9.99 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP OF008AH PPS - Branched
LNP* THERMOCOMP* OF008AH is a compound based on PPS - Branched resin containing 40% Glass Fiber. Added features of this grade are: Healthcare.
Izod Impact, Unnotched (ISO) 21.0 kJ/m²

@Temperature 23.0 °C
9.99 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Thermocomp OF008E PPS
LNP* Thermocomp* OF008E is a compound based on Polyphenylene Sulfide resin containing Glass Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the A..
Izod Impact, Unnotched (ISO) 21.0 kJ/m²
9.99 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP OF008E PPS - LINEAR
LNP* THERMOCOMP* OF008E is a compound based on PPS - Linear resin containing 40% Glass Fiber. Added features of this material include: Easy Molding.
Izod Impact, Unnotched (ISO) 21.0 kJ/m²
9.99 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP OF008E PPS (Asia Pacific)
LNP* Thermocomp* OF008E is a compound based on Polyphenylene Sulfide resin containing Glass Fiber. Added features of this material include: Easy Molding.
Izod Impact, Unnotched (ISO) 21.0 kJ/m²
9.99 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP RF002ES PA 66
LNP THERMOCOMP* RF002ES is a compound based on Nylon 66 resin containing 10% Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized.
Izod Impact, Unnotched (ISO) 21.0 kJ/m²
9.99 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP RF002SXS PA 66
LNP* THERMOCOMP* RF002SXS is a compound based on Nylon 66 resin contaning 10% Glass Fiber. Characteristcs of this grade are: Heat Stabilized.
Izod Impact, Unnotched (ISO) 21.0 kJ/m²

@Temperature -30.0 °C
9.99 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics Valox® SHF4910 PBT (Europe-Africa-Middle East)
6.5% glass reinforced, Super High Flow, flame retardant PBT.
Izod Impact, Unnotched (ISO) 21.0 kJ/m²
9.99 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP OF008A PPS - Branched
LNP* THERMOCOMP* OF008A is a compound based on PPS - Branched resin containing 40% Glass Fiber.
Izod Impact, Unnotched (ISO) >= 21.0 kJ/m²
>= 9.99 ft-lb/in²
Parallel to laminations; IEC 1212-2 5.5.3
Hippe SI GC 201 Woven Glass Cloth Reinforced Silicone Resin - Sheet
Used in electrical and electronic applications. Extremely good electrical properties under dry conditions; good properties under humid conditions.Information provided by Hippe.
Izod Impact, Unnotched (ISO) 21.0 kJ/m²
9.99 ft-lb/in²
80x10x4; ISO 180/1U
Eurostar Starpylen HW 30K ECR-BK PP, Injection Molded
Starpylen HW 30K ECR-BK is a reinforced Polypropylene with a low carbon footprint spherical filler, Injection Molding Resin (also known as HW30KECR)Information provided by Eurostar.
Izod Impact, Unnotched (ISO) 21.0 - 200 kJ/m²

@Temperature -20.0 - -20.0 °C
9.99 - 95.2 ft-lb/in²

@Temperature -4.00 - -4.00 °F
Average value: 72.5 kJ/m² Grade Count:4
Overview of materials for Polypropylene, Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Mineral Reinforced". Each property range of values reported is minimum and maximum values..