Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 21.0 kJ/m² | 9.99 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics Lexan® JK500 PC+ABS (Asia Pacific) 10% GR, ECO conforming FR, PC+ABS for thinwall molding applications. |
|||
Izod Impact, Unnotched (ISO) | 21.0 kJ/m² | 9.99 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP FARADEX NX07344 PC+ABS (Asia Pacific) Faradex NX07344 is a compound based on PC+ABS blend resin containing non-brominated and non-chlorinated flame retardant system, Stainless Steel and glass fiber. Added features of this material incl.. |
|||
Izod Impact, Unnotched (ISO) | 21.0 kJ/m² @Temperature -30.0 °C |
9.99 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP FARADEX NX07344 PC+ABS (Asia Pacific) Faradex NX07344 is a compound based on PC+ABS blend resin containing non-brominated and non-chlorinated flame retardant system, Stainless Steel and glass fiber. Added features of this material incl.. |
|||
Izod Impact, Unnotched (ISO) | 21.0 kJ/m² | 9.99 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP AL003 ABS LNP LUBRICOMP* AL003 is a compound based on Acrylonitrile Butadiene Styrene resin containing 15% PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Unnotched (ISO) | 21.0 kJ/m² | 9.99 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP AL003 ABS (Europe-Africa-Middle East) LNP LUBRICOMP* AL003 is a compound based on Acrylonitrile Butadiene Styrene resin containing PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Unnotched (ISO) | 21.0 kJ/m² - NB | 9.99 ft-lb/in² - NB | Average value: 96.6 kJ/m² Grade Count:64 |
Overview of materials for Polycarbonate/ABS Alloy, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Unreinforced". Each property range of values reported is minimum and maximum va.. |
|||
Izod Impact, Unnotched (ISO) | 21.0 - 52.0 kJ/m² @Temperature -40.0 - -30.0 °C |
9.99 - 24.7 ft-lb/in² @Temperature -40.0 - -22.0 °F |
Average value: 32.0 kJ/m² Grade Count:7 |
Overview of materials for Polycarbonate/ABS Alloy, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Glass Fiber Filled". Each property range of values reported is minimum and maxi.. |
|||
Izod Impact, Unnotched (ISO) | 21.0 kJ/m² - NB | 9.99 ft-lb/in² - NB | Average value: 24.5 kJ/m² Grade Count:8 |
Overview of materials for Polypropylene, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Molded". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Izod Impact, Unnotched (ISO) | 21.0 kJ/m² | 9.99 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP AL003 ABS (Asia Pacific) LNP LUBRICOMP* AL003 is a compound based on Acrylonitrile Butadiene Styrene resin containing PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Unnotched (ISO) | 21.0 kJ/m² | 9.99 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON Cycoloy_JK800 PC+ABS LNP* Stat-kon* Cycoloy_JK800 compound is an 8% carbon fiber reinforcedPC+ABS, electrostatic dissipative ECO conforming FR. Good hydrolytic stability. |
|||
Izod Impact, Unnotched (ISO) | 21.0 kJ/m² | 9.99 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON EX11402 PEI LNP* STAT-KON* EX11402 is a compound based on Polyetherimide resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive. |
|||
Izod Impact, Unnotched (ISO) | 21.0 kJ/m² | 9.99 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON OEL32 PPS - Linear LNP* STAT-KON* OCL32 is a compound based on PPS - Linear resin containing 10% Carbon Fiber, 15% PTFE. Added features of this grade include: Electrically Conductive, Wear Resistant. |
|||
Izod Impact, Unnotched (ISO) | 21.0 kJ/m² | 9.99 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP AF004L ABS LNP* THERMOCOMP* AF004L is a compound based on ABS resin containing 20% Glass Fiber. Added feature of this material is: Low Extractible. |
|||
Izod Impact, Unnotched (ISO) | 21.0 kJ/m² | 9.99 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_JK500 PC+ABS LNP* Thermocomp* Lexan_JK500 compound is a 10% GR, ECO conforming FR, PC+ABS for thinwall molding applications. |
|||
Izod Impact, Unnotched (ISO) | 21.0 kJ/m² | 9.99 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_JK500 PC+ABS (Asia Pacific) 10% GR, ECO conforming FR, PC+ABS for thinwall molding applications. |
|||
Izod Impact, Unnotched (ISO) | 21.0 kJ/m² | 9.99 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP OF008A PPS (Asia Pacific) LNP* Thermocomp* OF008A is a compound based on PPS - Branched resin containing Glass Fiber.This product is also known as Thermocomp* OF-1008. |
|||
Izod Impact, Unnotched (ISO) | 21.0 kJ/m² | 9.99 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP OF008AH PPS - Branched LNP* THERMOCOMP* OF008AH is a compound based on PPS - Branched resin containing 40% Glass Fiber. Added features of this grade are: Healthcare. |
|||
Izod Impact, Unnotched (ISO) | 21.0 kJ/m² @Temperature 23.0 °C |
9.99 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Thermocomp OF008E PPS LNP* Thermocomp* OF008E is a compound based on Polyphenylene Sulfide resin containing Glass Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the A.. |
|||
Izod Impact, Unnotched (ISO) | 21.0 kJ/m² | 9.99 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP OF008E PPS - LINEAR LNP* THERMOCOMP* OF008E is a compound based on PPS - Linear resin containing 40% Glass Fiber. Added features of this material include: Easy Molding. |
|||
Izod Impact, Unnotched (ISO) | 21.0 kJ/m² | 9.99 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP OF008E PPS (Asia Pacific) LNP* Thermocomp* OF008E is a compound based on Polyphenylene Sulfide resin containing Glass Fiber. Added features of this material include: Easy Molding. |
|||
Izod Impact, Unnotched (ISO) | 21.0 kJ/m² | 9.99 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP RF002ES PA 66 LNP THERMOCOMP* RF002ES is a compound based on Nylon 66 resin containing 10% Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized. |
|||
Izod Impact, Unnotched (ISO) | 21.0 kJ/m² | 9.99 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP RF002SXS PA 66 LNP* THERMOCOMP* RF002SXS is a compound based on Nylon 66 resin contaning 10% Glass Fiber. Characteristcs of this grade are: Heat Stabilized. |
|||
Izod Impact, Unnotched (ISO) | 21.0 kJ/m² @Temperature -30.0 °C |
9.99 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics Valox® SHF4910 PBT (Europe-Africa-Middle East) 6.5% glass reinforced, Super High Flow, flame retardant PBT. |
|||
Izod Impact, Unnotched (ISO) | 21.0 kJ/m² | 9.99 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP OF008A PPS - Branched LNP* THERMOCOMP* OF008A is a compound based on PPS - Branched resin containing 40% Glass Fiber. |
|||
Izod Impact, Unnotched (ISO) | >= 21.0 kJ/m² | >= 9.99 ft-lb/in² | Parallel to laminations; IEC 1212-2 5.5.3 |
Hippe SI GC 201 Woven Glass Cloth Reinforced Silicone Resin - Sheet Used in electrical and electronic applications. Extremely good electrical properties under dry conditions; good properties under humid conditions.Information provided by Hippe. |
|||
Izod Impact, Unnotched (ISO) | 21.0 kJ/m² | 9.99 ft-lb/in² | 80x10x4; ISO 180/1U |
Eurostar Starpylen HW 30K ECR-BK PP, Injection Molded Starpylen HW 30K ECR-BK is a reinforced Polypropylene with a low carbon footprint spherical filler, Injection Molding Resin (also known as HW30KECR)Information provided by Eurostar. |
|||
Izod Impact, Unnotched (ISO) | 21.0 - 200 kJ/m² @Temperature -20.0 - -20.0 °C |
9.99 - 95.2 ft-lb/in² @Temperature -4.00 - -4.00 °F |
Average value: 72.5 kJ/m² Grade Count:4 |
Overview of materials for Polypropylene, Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Mineral Reinforced". Each property range of values reported is minimum and maximum values.. |