Polymer Property : Izod Impact, Unnotched (ISO) = 25.7 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 54.0 kJ/m²
25.7 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP DFL14 PC
LNP LUBRICOMP* DFL14 is a compound based on Polycarbonate resin containing 20% Glass Fiber and 5% PTFE. Added features include: Internally Lubricated.
Izod Impact, Unnotched (ISO) 54.0 kJ/m²
25.7 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP GL003 PSU
LNP* Lubricomp* GL003 is a compound based on Polysulfone resin containing 15% PTFE. Added features of this material include: Internally Lubricated.
Izod Impact, Unnotched (ISO) 54.0 kJ/m²
25.7 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP GL003 PSU (Asia Pacific)
LNP* Lubricomp* GL003 is a compound based on Polysulfone resin containing PTFE. Added features of this material include: Internally Lubricated.
Izod Impact, Unnotched (ISO) 54.0 kJ/m²
25.7 ft-lb/in²
ISO 180/1eU
Solvay TECHNYLSTARâ„¢ S 60G1 V30 PA6, 30% glass filled, DRY
Description: TECHNYLSTARâ„¢ S 60G1 V30 is a reinforced 30% GF organophosphorous flame retarded grade based on a patented high flow polyamide 6 resin (TechnylStar). This product is heat stabilized..
Izod Impact, Unnotched (ISO) 54.0 kJ/m²
25.7 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP RFL36U PA 66
LNP* LUBRICOMP* RFL36U is a compound based on Nylon 66 resin containing 15% PTFE, 30% Glass Fiber. Added features of this grade include: Wear Resistant, UV Stabilized.
Izod Impact, Unnotched (ISO) 54.0 kJ/m²
25.7 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP STAT-KON RE004 PA 66
LNP* STAT-KON* RE004 is a compound based on Nylon 66 resin containing 20% Carbon Fiber. Added features of this material include: Electrically Conductive.
Izod Impact, Unnotched (ISO) 54.0 kJ/m²
25.7 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP DF002 PC
LNP THERMOCOMP* DF002 is a compound based on Polycarbonate resin containing 10% Glass Fiber.
Izod Impact, Unnotched (ISO) 54.0 kJ/m²
25.7 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP DF002H PC
LNP THERMOCOMP* DF002H is a compound based on Polycarbonate resin containing 10% Glass Fiber. Added feature includes: Healthcare.
Izod Impact, Unnotched (ISO) 54.0 kJ/m²
25.7 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP DF005 PC
LNP* Thermocomp* DF005 is a compound based on Polycarbonate containing 25% Glass Fiber.
Izod Impact, Unnotched (ISO) 54.0 kJ/m²
25.7 ft-lb/in²
80*10*3; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP DX06313I PC (Asia Pacific)
DX06313I is 30% glass fiber reinforced, impact modified polycarbonate resin. High flow and good ductility.
Izod Impact, Unnotched (ISO) 54.0 kJ/m²
25.7 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP LF003 PEEK
LNP* THERMOCOMP* LF003 is a compound based on Polyetheretherketone resin containing 15% Glass Fiber.
Izod Impact, Unnotched (ISO) 54.0 kJ/m²
25.7 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP LF003 PEEK (Asia Pacific)
LNP* Thermocomp* LF003 is a compound based on Polyetheretherketone resin containing Glass Fiber.
Izod Impact, Unnotched (ISO) 54.0 kJ/m²

@Temperature 23.0 °C
25.7 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Thermocomp LF003E PEEK
LNP* Thermocomp* LF003E is a compound based on Polyetheretherketone resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Unnotched (ISO) 54.0 kJ/m²

@Temperature 23.0 °C
25.7 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Thermocomp LF003E PEEK (Asia Pacific)
LNP* Thermocomp* LF003E is a compound based on Polyetheretherketone resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region.
Izod Impact, Unnotched (ISO) 54.0 kJ/m²

@Temperature 23.0 °C
25.7 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Thermocomp LF004 PEEK
LNP THERMOCOMP* LF004 is a compound based on Polyetheretherketone resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Unnotched (ISO) 54.0 kJ/m²

@Temperature -30.0 °C
25.7 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics NORYL BN9003G PPE+HIPS
PPE+PS blend. Unfilled. Blow molding. Excellent balance of impact and surface aesthetics. Suitable for automotive exterior components including spoilers.
Izod Impact, Unnotched (ISO) 54.0 kJ/m²
25.7 ft-lb/in²
DAM; ISO 180/1U
Solvay Technyl Starâ„¢ S 60G1 V30 30% Glass Reinforced Nylon 6, Flame Retardant
This Halogen free flame retardant grade, based on high fluidity Technyl Star, combines excellent all-round mechanical properties with outstanding flame retardancy and electrical performance. This pr..
Izod Impact, Unnotched (ISO) >= 54.0 kJ/m²
>= 25.7 ft-lb/in²
Parallel to laminations; IEC 1212-2 5.5.3
Hippe EP GC 205 Woven Glass Cloth Reinforced Epoxy Resin - Sheet
Used in mechanical, electrical and electronic applications. Extremely high mechanical strength at moderate temperature. Very good stability of electrical properties under high humidity. High mech..
Izod Impact, Unnotched (ISO) >= 54.0 kJ/m²
>= 25.7 ft-lb/in²
Parallel to laminations; IEC 1212-2 5.5.3
Hippe EP GM 202 Glass Mat Reinforced Epoxy Resin - Sheet
Izod Impact, Unnotched (ISO) >= 54.0 kJ/m²
>= 25.7 ft-lb/in²
Parallel to laminations; IEC 1212-2 5.5.3
Hippe EP GM 201 Glass Mat Reinforced Epoxy Resin - Sheet
Used in mechanical and electrical applications. Extremely high mechanical strength at moderate temperature. Very good electrical properties under high humidity.Information provided by Hippe.
Izod Impact, Unnotched (ISO) >= 54.0 kJ/m²
>= 25.7 ft-lb/in²
Parallel to laminations; IEC 1212-2 5.5.3
Hippe EP GM 203 Glass Mat Reinforced Epoxy Resin - Sheet
Izod Impact, Unnotched (ISO) >= 54.0 kJ/m²
>= 25.7 ft-lb/in²
Parallel to laminations; IEC 1212-2 5.5.3
Hippe EP GM 204 Glass Mat Reinforced Epoxy Resin - Sheet
Izod Impact, Unnotched (ISO) 54.0 kJ/m²
25.7 ft-lb/in²
80x10x4; ISO 180/1U
Eurostar Starflam PF0057E PA6, 25% Glass Filled, Injection Molded
Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 6 Injection Molding Resin (also known as PF-1005 Z270)Information provided by Polymer Technology & Services,..
Izod Impact, Unnotched (ISO) 54.0 kJ/m²
25.7 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP JF002 PES
LNP THERMOCOMP* JF002 is a compound based on Polyethersulfone resin containing 10% Glass Fiber.