Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 70.0 kJ/m² | 33.3 ft-lb/in² | 80*10*3; ISO 180/1U |
SABIC Innovative Plastics Lexan® IFX5420Z PC (Asia Pacific) Lexan* IFX5420Z is a medium viscosity, release containing, injection moldable polycarbonate grade suitable for use in industry protective eye-ware welding applications. This grade meets the transmis.. |
|||
Izod Impact, Unnotched (ISO) | 70.0 kJ/m² | 33.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP FARADEX DS0036I PC (Europe-Africa-Middle East) LNP* Faradex* DS0036I is a compound based on Polycarbonate resin containing Flame Retardant, Stainless Steel Fiber. Added features of this material include: High Impact, Flame Retardant, Non-Bromin.. |
|||
Izod Impact, Unnotched (ISO) | 70.0 kJ/m² @Temperature 23.0 °C |
33.3 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Faradex DS0036IC PC (Europe-Africa-Middle East) LNP* FARADEX* DS0036IC is a compound based on Polycarbonate resin, containing Stainless Steel Fiber, Flame Retardant. Added features include: Non-Brominated & Non-Chlorinated Flame Retardant, High I.. |
|||
Izod Impact, Unnotched (ISO) | 70.0 kJ/m² | 33.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP FARADEX NX07330 PC+ABS (Asia Pacific) Faradex NX07330 is a compound based on PC+ABS blend resin containing stainless steel and glass fiber. Added features of this material include EMI/RFI Shielding and ESD. |
|||
Izod Impact, Unnotched (ISO) | 70.0 kJ/m² | 33.3 ft-lb/in² | DIN 53453 |
Ineos Nova S-5400 High Impact Compact Polystyrene
(discontinued **) Impact polystyrene with high dimensional stability under heat, particularly suitable fore extrusion and thermoforming of technical parts or packaging applications but also used for injection molding.. |
|||
Izod Impact, Unnotched (ISO) | 70.0 kJ/m² @Temperature 23.0 °C |
33.3 ft-lb/in² @Temperature 73.4 °F |
ISO 180/U |
Victrex® PEEK -HT™ 22GL30 Polyetherketone, 30% Glass Fiber Reinforced Product Description:High performance thermoplastic material, 30% glass fibre reinforced PolyEtherKetone (PEK), semi crystalline, granules for injection moulding, standard flow, FDA food contact comp.. |
|||
Izod Impact, Unnotched (ISO) | 70.0 kJ/m² - NB | 33.3 ft-lb/in² - NB | Average value: 70.0 kJ/m² Grade Count:9 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant". Each property range of values rep.. |
|||
Izod Impact, Unnotched (ISO) | 70.0 kJ/m² - NB | 33.3 ft-lb/in² - NB | Average value: 89.9 kJ/m² Grade Count:19 |
Overview of materials for Nylon 6, 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. E.. |
|||
Izod Impact, Unnotched (ISO) | 70.0 kJ/m² | 33.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP RFL36 PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RFL36 is a compound based on Nylon 66 resin containing Glass Fiber, PTFE. |
|||
Izod Impact, Unnotched (ISO) | 70.0 kJ/m² | 33.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP RFL36SXD PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RFL36SXD is a compound based on Nylon 66 resin containing Glass Fiber, PTFE. Added features of this material include: Heat Stabilized. |
|||
Izod Impact, Unnotched (ISO) | 70.0 kJ/m² | 33.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP UFL36S PPA LNP LUBRICOMP* UFL36S is a compound based on Polyphthalamide resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Heat Stabilized, Wear Resistant, Bearing Grade. |
|||
Izod Impact, Unnotched (ISO) | 70.0 kJ/m² | 33.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP UFL36SXC PPA (Asia Pacific) LNP* Lubricomp* UFL36SXC is a compound based on Polyphthalamide resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated, Heat Stabilized. |
|||
Izod Impact, Unnotched (ISO) | 70.0 kJ/m² | 33.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP UFL36SXQ PPA (Asia Pacific) LNP* Lubricomp* UFL36SXQ is a compound based on Polyphthalamide resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated, Heat Stabilized. |
|||
Izod Impact, Unnotched (ISO) | 70.0 kJ/m² | 33.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON DD0009XP PC (Asia Pacific) LNP* Stat-kon* DD0009XP is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include:Electrically Conductive, Flame Retardant. Also known as Stat-Kon*.. |
|||
Izod Impact, Unnotched (ISO) | 70.0 kJ/m² | 33.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP RC008ESS PA 66 (Europe-Africa-Middle East) LNP* THERMOCOMP* RC008ESS is a compound based on PA66 resin containing Carbon Fiber. Added features include; Electrically Conductive, Easy Molding, Heat Stabilized. |
|||
Izod Impact, Unnotched (ISO) | 70.0 kJ/m² @Temperature 23.0 °C |
33.3 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Thermocomp RF008U PA 66 (Europe-Africa-Middle East) LNP* THERMOCOMP* RF008U is a compound based on PA 66 resin containing Glass Fiber. Added features include; UV-Stabilized, Easy Molding.This data was supplied by SABIC-IP for the Europe-Africa-Middle.. |
|||
Izod Impact, Unnotched (ISO) | 70.0 kJ/m² @Temperature 23.0 °C |
33.3 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Thermotuf PK005EI2 PA 6 (Europe-Africa-Middle East) LNP* THERMOTUF* PK005EI2 is a compound based on PA 6 resin containing Impact Modifier, Mineral. Added features include: High Impact.This data was supplied by SABIC-IP for the Europe-Africa-Middle Ea.. |
|||
Izod Impact, Unnotched (ISO) | 70.0 kJ/m² | 33.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP VERTON UX03320 PPA (Europe-Africa-Middle East) VERTON* UX03320 is a compound based on Polyphthalamide resin containing Long Glass. |
|||
Izod Impact, Unnotched (ISO) | 70.0 kJ/m² | 33.3 ft-lb/in² | 80x10x4; ISO 180/1U |
Eurostar Staramide RF008U PA66/6, 40% Glass Filled, Injection Molded Staramide RF008U is a 40% Glass Fiber Reinforced Polyamide 66/Polyamide 6 Injection Molding Resin (also known as Staramide 66 C 40V S4)Information provided by Eurostar. |
|||
Izod Impact, Unnotched (ISO) | 70.0 kJ/m² | 33.3 ft-lb/in² | 80x10x4; ISO 180/1U |
Eurostar Starpylen MK001AS PP, Mineral Filled, Injection Molding Starpylen MK001AS is a Mineral Filled Polypropylene Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Unnotched (ISO) | 70.0 kJ/m² | 33.3 ft-lb/in² | 80x10x4; ISO 180/1U |
Eurostar Staramide PK005EI2 PA6, Mineral Fiber Filled, Impact Modified Injection Molded Staramide PK005EI2 is an Impact Modified Mineral Filled Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Unnotched (ISO) | 70.0 kJ/m² | 33.3 ft-lb/in² | ASTM D256 |
Beijing Ranger Chem PBT 403 G-M50 Heat Resistant and Environmental Protection Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Izod Impact, Unnotched (ISO) | 70.0 - 70.0 kJ/m² @Temperature -30.0 - -30.0 °C |
33.3 - 33.3 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 70.0 kJ/m² Grade Count:1 |
Overview of materials for Nylon 66, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, PTFE Filled". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Izod Impact, Unnotched (ISO) | 70.0 kJ/m² @Temperature 23.0 °C |
33.3 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Verton PV007SV_YW8D151 PA 6 Preliminary data for 35% long fiber single pellet color filled PA6This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Unnotched (ISO) | 70.0 kJ/m² | 33.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP VERTON RVL36SXS PA 66 (Europe-Africa-Middle East) LNP* VERTON* RVL36SXS is a compound based on PA 66 resin containing Long Glass Fiber, PTFE. Added features include; Internally Lubricated. |
|||
Izod Impact, Unnotched (ISO) | 70.0 kJ/m² | 33.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP VERTON RX00078 PA 66 (Europe-Africa-Middle East) LNP* VERTON* RX00078 is a compound based on PA 66 resin containing Long Glass Fiber, Proprietary Lubricant. Added features include: Internally Lubricated. |
|||
Izod Impact, Unnotched (ISO) | 70.0 kJ/m² | 33.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP VERTON UX03320 PPA (Asia Pacific) VERTON* UX03320 is a compound based on Polyphthalamide resin containing Long Glass. |
|||
Izod Impact, Unnotched (ISO) | 70.0 kJ/m² | 33.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics NORYL PX2060 PPE+PS (Asia Pacific) Noryl* PX2060 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR .. |
|||
Izod Impact, Unnotched (ISO) | 70.0 kJ/m² | 33.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics NORYL PX2060 PPE+PS (Europe-Africa-Middle East) Noryl* PX2060 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR .. |
|||
Izod Impact, Unnotched (ISO) | 70.0 kJ/m² | 33.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics NORYL PX2060 PPE+PS Noryl* PX2060 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR .. |