Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP FARADEX DS0036I PC (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP FARADEX
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP FARADEX DS0036I PC (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Faradex* DS0036I is a compound based on Polycarbonate resin containing Flame Retardant, Stainless Steel Fiber. Added features of this material include: High Impact, Flame Retardant, Non-Brominated & Non-Chlorinated Flame Retardant, EMI/RFI Shielding.
Physical Properties Metric English Comments
Density 1.29 g/cc
0.0466 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0040 - 0.0070 cm/cm
0.0040 - 0.0070 in/in
on Tensile Bar; SABIC Method
Linear Mold Shrinkage, Transverse 0.0040 - 0.0060 cm/cm

@Time 86400 sec
0.0040 - 0.0060 in/in

@Time 24.0 hour
ISO 294
Mechanical Properties Metric English Comments
Tensile Strength at Break 55.0 MPa
7980 psi
5 mm/min; ISO 527
Tensile Strength, Yield 57.0 MPa
8270 psi
5 mm/min; ISO 527
Elongation at Break 4.0 - 8.0 %
4.0 - 8.0 %
5 mm/min; ISO 527
Elongation at Yield 3.8 %
3.8 %
5 mm/min; ISO 527
Tensile Modulus 2.50 GPa
363 ksi
1 mm/min; ISO 527
Flexural Yield Strength 80.0 MPa
11600 psi
2 mm/min; ISO 178
Flexural Modulus 2.60 GPa
377 ksi
2 mm/min; ISO 178
Izod Impact, Notched 1.25 J/cm
2.34 ft-lb/in
ASTM D256
Izod Impact, Unnotched 17.9 J/cm
33.5 ft-lb/in
ASTM D4812
Izod Impact, Notched (ISO) 10.0 kJ/m²
4.76 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 70.0 kJ/m²
33.3 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 57.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
31.7 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow 68.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
37.8 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 136 °C
277 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 125 °C
257 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
Flammability, UL94 V-0

@Thickness 2.00 mm
V-0

@Thickness 0.0787 in
UL 94
Electrical Properties Metric English Comments
Volume Resistivity 10000 - 1.00e+6 ohm-cm
10000 - 1.00e+6 ohm-cm
ASTM D257
Surface Resistance 100 - 10000 ohm
100 - 10000 ohm
ASTM D257
Shielding Effectiveness 40 - 55 dB

@Thickness 3.00 mm
40 - 55 dB

@Thickness 0.118 in
SABIC Method