Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 80.0 kJ/m² | 38.1 ft-lb/in² | 80*10*3; ISO 180/1U |
SABIC Innovative Plastics Lexan® BFL2015 PC Non-brominated, non-chlorinated flame retardant, glass reinforced PC. Opaque colors only |
|||
Izod Impact, Unnotched (ISO) | 80.0 kJ/m² @Temperature -30.0 °C |
38.1 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1U |
SABIC Innovative Plastics Lexan® BFL2015 PC Non-brominated, non-chlorinated flame retardant, glass reinforced PC. Opaque colors only |
|||
Izod Impact, Unnotched (ISO) | 80.0 kJ/m² @Temperature -30.0 °C |
38.1 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1U |
SABIC Innovative Plastics Lexan® BFL2015 PC (Asia Pacific) Non-brominated, non-chlorinated flame retardant, glass reinforced PC. Opaque colors only |
|||
Izod Impact, Unnotched (ISO) | 80.0 kJ/m² | 38.1 ft-lb/in² | 80*10*3; ISO 180/1U |
SABIC Innovative Plastics Lexan® BFL2015 PC (Europe-Africa-Middle East) Non-brominated, non-chlorinated flame retardant, glass reinforced PC. Opaque colors only |
|||
Izod Impact, Unnotched (ISO) | 80.0 kJ/m² | 38.1 ft-lb/in² | 80*10*3; ISO 180/1U |
SABIC Innovative Plastics Lexan® BFL2015HF PC (Asia Pacific) Non-brominated, non-chlorinated flame retardant, glass reinforced PC. Opaque colors only. UL94 V0 1.5 mm for BLACK; V1 1.5 mm for OTHER Color. |
|||
Izod Impact, Unnotched (ISO) | 80.0 kJ/m² | 38.1 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP FARADEX MS003 PP LNP* FARADEX* MS003 is a compound based on Polypropylene resin containing 15% Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Izod Impact, Unnotched (ISO) | 80.0 kJ/m² | 38.1 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP FARADEX MS003 PP (Europe-Africa-Middle East) LNP* Faradex* MS003 is a compound based on Polypropylene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Izod Impact, Unnotched (ISO) | 80.0 kJ/m² - NB | 38.1 ft-lb/in² - NB | Average value: 109 kJ/m² Grade Count:6 |
Overview of materials for Polybutylene Terephthalate (PBT), Unreinforced, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Unreinforced, Molded". Each property range of values reported is minim.. |
|||
Izod Impact, Unnotched (ISO) | 80.0 kJ/m² @Temperature -30.0 °C |
38.1 ft-lb/in² @Temperature -22.0 °F |
|
Polimeri Europa KOBLEND HI PD 41 G1 PBT+PC, 5% Glass Fiber
(discontinued **) Symbol according to ISO 1043/1: PBT+PC (GF) Elastomer modified PBT+PC blend reinforced with 5% of glass fibres, a good combination of stiffness, dimensional stability and thoughness. Main applicat.. |
|||
Izod Impact, Unnotched (ISO) | 80.0 - 100 kJ/m² @Temperature -30.0 - -30.0 °C |
38.1 - 47.6 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 95.7 kJ/m² Grade Count:7 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded". Each property range of values reported is .. |
|||
Izod Impact, Unnotched (ISO) | 80.0 - 100 kJ/m² | 38.1 - 47.6 ft-lb/in² | Average value: 85.0 kJ/m² Grade Count:4 |
Overview of materials for Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded". Each property range of values reported is m.. |
|||
Izod Impact, Unnotched (ISO) | 80.0 - 103 kJ/m² | 38.1 - 49.0 ft-lb/in² | Average value: 90.6 kJ/m² Grade Count:5 |
Overview of materials for Nylon 66, 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. .. |
|||
Izod Impact, Unnotched (ISO) | 80.0 kJ/m² | 38.1 ft-lb/in² | ISO 180/1eU |
Solvay TECHNYL® A 218HP V50 PA66, 35% glass fiber, DRY Description: TECHNYL® A 218HP V50 is a polyamide 66, reinforced with 50% of glass fiber, heat stabilized, for injection molding. This product is available in black color.Benefits: The product off.. |
|||
Izod Impact, Unnotched (ISO) | 80.0 kJ/m² | 38.1 ft-lb/in² | ISO 180/1eU |
Solvay TECHNYLSTARâ„¢ S 216 V35 PA6, 35% glass filled, Conditioned Description: TECHNYLSTAR polyamide, reinforced with 35% of glass fiber, for injection molding. Characterized by a high fluidity of the melt.Available in: Europe and North AmericaProduct Applications.. |
|||
Izod Impact, Unnotched (ISO) | 80.0 kJ/m² | 38.1 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP RFL36S PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RFL36S is a compound based on Nylon 66 resin containing Glass Fiber, PTFE. Added features of this material include: Heat Stabilized. |
|||
Izod Impact, Unnotched (ISO) | 80.0 kJ/m² | 38.1 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP RFN18 PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RFN18 is a compound based on Nylon 66 resin containing Glass Fiber, MOS2. |
|||
Izod Impact, Unnotched (ISO) | 80.0 kJ/m² @Temperature 23.0 °C |
38.1 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Thermocomp RF006EU PA 66 (Europe-Africa-Middle East) LNP* THERMOCOMP* RF006EU is a compound based on PA 66 resin containing Glass Fiber. Added features include: Easy Molding, UV-StabilizedThis data was supplied by SABIC-IP for the Europe-Africa-Middle.. |
|||
Izod Impact, Unnotched (ISO) | 80.0 kJ/m² | 38.1 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP RF00ASXS PA6.6 (Europe-Africa-Middle East) LNP* Thermocomp* RF00ASXS is a compound based on PA 66 resin containing Glass Fiber. Added features include: Heat Stabilized. |
|||
Izod Impact, Unnotched (ISO) | 80.0 kJ/m² | 38.1 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP YF006A Polyester Elastomer (Europe-Africa-Middle East) LNP* THERMOCOMP* YF006A is a compound based on Polyester Elastomer containing Glass Fiber. |
|||
Izod Impact, Unnotched (ISO) | 80.0 kJ/m² | 38.1 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON DX05305C PC LNP* STAT-KON* DX05305C is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive, Clean Compounding System. |
|||
Izod Impact, Unnotched (ISO) | 80.0 kJ/m² | 38.1 ft-lb/in² | 50%RH; ISO 180/1U |
DuPont Performance Polymers Zytel® 80G33L NC010 Nylon 66
(Unverified Data**) 33% Glass Reinforced Toughened Polyamide 66 Zytel 80G33L NC010 is a 33% glass fiber reinforced polyamide 66 resin with outstanding impact resistance developed using DuPont Super Tough technology.Inf.. |
|||
Izod Impact, Unnotched (ISO) | 80.0 kJ/m² | 38.1 ft-lb/in² | 80x10x4; ISO 180/1U |
Eurostar Staramide RF00ASXS PA66, 50% Glass Filled, Injection Molded Staramide RF00ASXA is a 50% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Unnotched (ISO) | 80.0 kJ/m² | 38.1 ft-lb/in² | ISO 180/1C |
Chi Mei Polylac® PA-756H ABS - High Flow Super high flow |
|||
Izod Impact, Unnotched (ISO) | 80.0 kJ/m² | 38.1 ft-lb/in² | 80x10x4; ISO 180/1U |
Eurostar Star L PA66 30V D51 PA66, Glass Fiber Filled, Injection Molded Star L PA66 30V D51 is a PTFE lubricated, Glass Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Unnotched (ISO) | 80.0 kJ/m² | 38.1 ft-lb/in² | 80x10x4; ISO 180/1U |
Eurostar Staramide RF006EU PA66/6, Glass Fiber Filled, Injection Molded Staramide RF006EU is an UV stabilized, Glass Fiber Reinforced Polyamide 66/Polyamide 6 Injection Molding Resin (also known as Staramide 66C 30V S4)Information provided by Eurostar. |
|||
Izod Impact, Unnotched (ISO) | 80.0 kJ/m² | 38.1 ft-lb/in² | ASTM D256 |
BLUESTAR 101G0 PBT Typical Applications: Appliance, partsInformation provided by Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Unnotched (ISO) | 80.0 kJ/m² | 38.1 ft-lb/in² | 80*10*3; ISO 180/1U |
SABIC Innovative Plastics Lexan® ML3260 PC (Europe-Africa-Middle East) LEXAN ML3260 is a medium viscosity, 15% glass reinforced, flame retardant grade especially designed for applications like computer cartridges. |
|||
Izod Impact, Unnotched (ISO) | 80.0 kJ/m² | 38.1 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP FP003 PE (Europe-Africa-Middle East) LNP *Lubricomp* FP003 is a compound based on Polyethylene resin, containing PTFE and Silicone. Added features include: Internally Lubricated. |
|||
Izod Impact, Unnotched (ISO) | 80.0 kJ/m² @Temperature -30.0 °C |
38.1 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics Xenoy® X5630P PET+PC (Europe-Africa-Middle East) Mineral filled PC/PET blend with high heat dimensional stability, low shrinkage and low CTE, especially for painted applications |