Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 3.00 - 22.0 kJ/m²

@Temperature -40.0 - -30.0 °C
1.43 - 10.5 ft-lb/in²

@Temperature -40.0 - -22.0 °F
Average value: 7.20 kJ/m² Grade Count:6
Overview of materials for Polybutylene Terephthalate (PBT), Unreinforced, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Unreinforced, Molded". Each property range of values reported is minim..
Izod Impact, Notched (ISO) 7.00 - 22.0 kJ/m²

@Temperature -30.0 - -20.0 °C
3.33 - 10.5 ft-lb/in²

@Temperature -22.0 - -4.00 °F
Average value: 13.1 kJ/m² Grade Count:10
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Extruded". Each property range of values reported is minimum and ..
Izod Impact, Notched (ISO) 6.20 - 22.0 kJ/m²
2.95 - 10.5 ft-lb/in²
Average value: 12.0 kJ/m² Grade Count:12
Overview of materials for Nylon 66/6, 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are incl..