Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 17.0 kJ/m² @Thickness 4.00 mm, Temperature 23.0 °C |
8.09 ft-lb/in² @Thickness 0.157 in, Temperature 73.4 °F |
ISO 180/1A |
Polimeri Europa Sinkral® C 442 ABS Resin Sinkral C 442 is a heat resistant injection molding grade offering good flow and impact resistance together with excellent thermal stability during processing. Designation: Thermoplastic ISO 2580-AB.. |
|||
Izod Impact, Notched (ISO) | 17.0 kJ/m² @Temperature 23.0 °C |
8.09 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Geloy HRA222 ASA (Europe-Africa-Middle East) GELOY HRA222 is a multi-purpose, chlorine and bromine free flame retardant ASA+PC alloy for injection moulding processes. Typical properties as measured on natural material.This data was supplied by.. |
|||
Izod Impact, Notched (ISO) | 17.0 kJ/m² @Temperature -30.0 °C |
8.09 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Geloy XTPM307 ASA+PC (Europe-Africa-Middle East) XTPM307 is a high heat resistant PC/ASA with improved processing stability over HRA150. Typical values measured on natural material.This data was supplied by SABIC-IP for the Europe-Africa-Middle Ea.. |
|||
Izod Impact, Notched (ISO) | 17.0 kJ/m² @Temperature 23.0 °C |
8.09 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Nilit Nilamid B3 H G10 50% Glass Fiber Reinforced PA6 Description: Nilamid B3 H G10 is a product that combines outstanding strength and stiffness with good moldability and good impact strength. It is widely used for structural applications.Key characte.. |
|||
Izod Impact, Notched (ISO) | 17.0 kJ/m² @Temperature 23.0 °C |
8.09 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 180/1A |
DuPont Performance Polymers Zytel® 73G30T BK261 Nylon 6
(Unverified Data**) Zytel® 73G30T BK261 is a 30% glass fiber reinforced, toughened, black polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Notched (ISO) | 17.0 kJ/m² @Temperature 23.0 °C |
8.09 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 180/1A |
DuPont Performance Polymers Zytel® 73G30T NC010 Nylon 6
(Unverified Data**) Zytel® 73G30T NC010 is a 30% glass fiber reinforced, toughened polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Notched (ISO) | 17.0 kJ/m² @Temperature 23.0 °C |
8.09 ft-lb/in² @Temperature 73.4 °F |
ISO 180-1A |
Ineos ABS Lustran® ABS 450 Injection Molding Grade Lustran® ABS 450 has medium impact strength, high flow, and is injection molding grade. |
|||
Izod Impact, Notched (ISO) | 17.0 kJ/m² @Temperature -30.0 °C |
8.09 ft-lb/in² @Temperature -22.0 °F |
ISO 180-1A |
Lanxess Pocan® DP C 1502 000000 PBT + PC PBT + PC, non-reinforced, injection molding, improved impact strength, low tendency to warp, UV-stabilizedInformation provided by LANXESS. |
|||
Izod Impact, Notched (ISO) | 17.0 kJ/m² @Temperature -20.0 °C |
8.09 ft-lb/in² @Temperature -4.00 °F |
ISO 180-1A |
Ineos ABS Lustran® ABS 970 Lustran® ABS 970 has high impact strength and good paintability. |
|||
Izod Impact, Notched (ISO) | 17.0 kJ/m² @Temperature -30.0 °C |
8.09 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Xylex X7503HP PC+POLYESTER (Europe-Africa-Middle East) Clear PC-Siloxane copolymer + Polyester alloy, USA Food ContactThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched (ISO) | 17.0 kJ/m² @Temperature 23.0 °C |
8.09 ft-lb/in² @Temperature 73.4 °F |
ISO 180/A |
Styrolution Novodur® H605 ABS Novodur H605 is a high heat injection molding grade with enhanced flowability and reduced emission.Information provided by Styrolution |
|||
Izod Impact, Notched (ISO) | 17.0 kJ/m² @Temperature 23.0 °C |
8.09 ft-lb/in² @Temperature 73.4 °F |
ISO 180/A |
Styrolution Novodur® H702 ABS Novodur H702 is a high heat, high gloss injection molding grade with very good flowabilityInformation provided by Styrolution |
|||
Izod Impact, Notched (ISO) | 17.0 kJ/m² @Temperature 23.0 °C |
8.09 ft-lb/in² @Temperature 73.4 °F |
ISO 180/A |
Styrolution Novodur® H950 ABS Novodur H950 is a very high heat injection molding grade with high gloss surface appearanceInformation provided by Styrolution |
|||
Izod Impact, Notched (ISO) | 17.0 kJ/m² @Temperature 23.0 °C |
8.09 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Styron MAGNUMâ„¢ 3325 MT Acrylonitrile Butadiene Styrene (ABS) Resin Overview: MAGNUMâ„¢ 3325 MT is a resin with excellent processing characteristics and matt surface finish. The mass (continuous process) ABS technology of Styron ensures an ABS resin that combines.. |
|||
Izod Impact, Notched (ISO) | 17.0 kJ/m² @Temperature -30.0 °C |
8.09 ft-lb/in² @Temperature -22.0 °F |
ISO 180/A |
Styron Magnumâ„¢ 3904 Acrylonitrile Butadiene Styrene (ABS) MAGNUMâ„¢ 3904 is a resin with super-high impact. It is used in a wide range of technical applications. The mass (continuous process) ABS technology of Dow ensures an ABS resin that combines ex.. |
|||
Izod Impact, Notched (ISO) | 17.0 kJ/m² @Temperature -30.0 °C |
8.09 ft-lb/in² @Temperature -22.0 °F |
Injection Molded; ISO 180/A |
Styron MAGNUMâ„¢ 3904 Smooth Acrylonitrile Butadiene Styrene (ABS) Resin Overview: MAGNUMâ„¢ 3904 is an extrusion/thermoforming resin developed for high impact and other technical applications. The mass (continuous process) ABS technology of Styron ensures an ABS tech.. |
|||
Izod Impact, Notched (ISO) | 17.0 kJ/m² @Temperature -30.0 °C |
8.09 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Noryl GTX GTX9200 PPE+PS+PA66 High Flow GTX for Automotive applicationsThis data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched (ISO) | 17.0 kJ/m² @Temperature -30.0 °C |
8.09 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Noryl GTX GTX9200 PPE+PS+PA66 (Asia Pacific) High Flow GTX for Automotive applicationsThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched (ISO) | 17.0 kJ/m² @Temperature 23.0 °C |
8.09 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Noryl GTX GTX976 PPE+PA (Europe-Africa-Middle East) NORYL GTX976 is a material especially designed for electrostatic painting and powder coating applications. This material combines high impact performance with conductivity in an unique way.This data.. |
|||
Izod Impact, Notched (ISO) | 17.0 kJ/m² @Temperature 23.0 °C |
8.09 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Noryl GTX GTX979 PPE+PA NORYL GTX979 is a conductive, high heat material. It is especially designed for in- and on-line painted bodypanels and fenders in particular, with conductivity for electro-static painting in an uniq.. |
|||
Izod Impact, Notched (ISO) | 17.0 kJ/m² @Temperature 23.0 °C |
8.09 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Noryl GTX GTX979 PPE+PA (Europe-Africa-Middle East) NORYL GTX979 is a conductive, high heat material. It is especially designed for in- and on-line painted bodypanels and fenders in particular, with conductivity for electro-static painting in an uniq.. |
|||
Izod Impact, Notched (ISO) | 17.0 kJ/m² @Temperature 23.0 °C |
8.09 ft-lb/in² @Temperature 73.4 °F |
ISO 180/A |
Styron Magnumâ„¢ 3325 MT Acrylonitrile Butadiene Styrene (ABS) MAGNUMâ„¢ 3325 MT is resin with excellent processing characteristics and a matt surface finish. The mass (continuous process) ABS technology of Dow ensures an ABS resin that combines excellent p.. |
|||
Izod Impact, Notched (ISO) | 17.0 kJ/m² @Temperature -30.0 °C |
8.09 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Noryl MX5569 PPE+PS PPE+PS blend. High Heat. Good balance of flow and impact. Offers good aging performance under heat. Typical applications include Automotive Interiors and Lighting.This data was supplied by SABIC-.. |
|||
Izod Impact, Notched (ISO) | 17.0 kJ/m² @Temperature 23.0 °C |
8.09 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Borealis Daplen™ KB4436 Polypropylene TPO Compound Daplen™ KB4436 is a 30% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and gi.. |
|||
Izod Impact, Notched (ISO) | 17.0 kJ/m² @Temperature 23.0 °C |
8.09 ft-lb/in² @Temperature 73.4 °F |
80x10x4; ISO 180/1A |
Eurostar Staramide BG8 PA6, 40% Glass Fiber Filled, Injection Molded Staramide BG8 is a 40% Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Notched (ISO) | 17.0 kJ/m² @Temperature -30.0 °C |
8.09 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Eurotec® Tecomid® NA40 GR30 NL IH PA6.6, 30% glass fiber reinforced, impact modified, natural Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 17.0 kJ/m² @Temperature -30.0 °C |
8.09 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Eurotec® Tecomid® NB40 GR50 NL PA 6 50% glass fiber reinforced Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Izod Impact, Notched (ISO) | 17.0 kJ/m² @Temperature 23.0 °C |
8.09 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Eurotec® Tecomid® NB40 NL IX PA6, impact modified, natural Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 17.0 kJ/m² @Temperature 23.0 °C |
8.09 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 180/1A |
DuPont Performance Polymers Zytel® 77G43L NC010 Nylon 612
(Unverified Data**) Zytel® 77G43L NC010 is a 43% glass fiber reinforced polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Notched (ISO) | 17.0 kJ/m² @Temperature 23.0 °C |
8.09 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® SD9705 PC Copolymer (Europe-Africa-Middle East) High visocisty PC Copolymer, low smoke, flame retardant resinThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |