Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 4.50 kJ/m²

@Temperature 23.0 °C
2.14 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1A
Nilit Nilamid B3N Unfilled, Nucleated PA6
Description: Nilamid B3N is an unfilled, nucleated NYLON 6. It is fast cycling, and combines ease of processing with good overall mechanical characteristics.Key characteristics: Fast cyclingEasy pro..
Izod Impact, Notched (ISO) 4.50 kJ/m²

@Temperature 23.0 °C
2.14 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1A
DuPont Performance Polymers Crastin® FG6129 NC010 PBT  (Unverified Data**)
Crastin® FG6129 NC010 is an unreinforced, high viscosity polybutylene terephthalate resin for extrusion and injection molding. It has been developed for consideration into applications such as part..
Izod Impact, Notched (ISO) 4.50 kJ/m²

@Temperature 23.0 °C
2.14 ft-lb/in²

@Temperature 73.4 °F
ISO 180
Eastman 9921 PET Injection Molded  (discontinued **)
VORIDIAN polymer 9921 is a copolymer PET that has been crystallized. Color concentrates of polymer 9921 are available on request.Applications/UsesAutomotive parts containersFood packagingHousehold p..
Izod Impact, Notched (ISO) 4.50 kJ/m²

@Thickness 3.17 mm,
Temperature -40.0 °C
2.14 ft-lb/in²

@Thickness 0.125 in,
Temperature -40.0 °F
ISO 180
Phillips Sumika Marlex® ABF-300 High Flow Thermoplastic Olefin  (discontinued **)
Applications: Automotive exterior fasciasInformation provided by Chevron Phillips.Phillips Sumika Polypropylene Company has been shut down, as announced in 2011.
Izod Impact, Notched (ISO) 4.50 kJ/m²

@Temperature 23.0 °C
2.14 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1A
Nilit Nilamid A3 N H2 Nucleated, Heat Stabilized Nylon 66
Description: Nilamid A3 N H2 is a nucleated, heat stabilized NYLON 66 with excellent flow characteristics and very fast cycle time. It is widely used throughout many industries for mass production a..
Izod Impact, Notched (ISO) 4.50 kJ/m²

@Temperature -30.0 °C
2.14 ft-lb/in²

@Temperature -22.0 °F
DAM; ISO 180/1A
DuPont Performance Polymers Zytel® 151 NC010 Nylon 612  (Unverified Data**)
Zytel® 151 NC010 is a PA 612 resin.Information provided by DuPont Performance Polymers
Izod Impact, Notched (ISO) 4.50 kJ/m²

@Temperature 23.0 °C
2.14 ft-lb/in²

@Temperature 73.4 °F
50%RH; ISO 180/1A
DuPont Performance Polymers Zytel® 151 NC010 Nylon 612  (Unverified Data**)
Zytel® 151 NC010 is a PA 612 resin.Information provided by DuPont Performance Polymers
Izod Impact, Notched (ISO) 4.50 kJ/m²

@Temperature 23.0 °C
2.14 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Inno-Comp INNOPOL® CS 1-3250 42% Chalk-Filled Polypropylene Homopolymer
INNOPOL® CS 1-3250 is a 42% chalk-filled polypropylene homopolymer compound /PP-H KD42 (ISO 1043)/. This grade is available in natural and custom colored form.INNOPOL® CS 1-3250 is developed f..
Izod Impact, Notched (ISO) 4.50 kJ/m²

@Temperature -40.0 °C
2.14 ft-lb/in²

@Temperature -40.0 °F
ISO 180
LyondellBasell Hostacomâ„¢ CB267 Thermoplastic Polyolefin Elastomer
Description: Hostacomâ„¢ CB267 medium melt flow, 1,600 MPa flexural modulus thermoplastic elastomeric olefin (TEO) resin has an excellent balance of scratch and mar resistance, rigidity and impac..
Izod Impact, Notched (ISO) 4.50 kJ/m²

@Temperature -20.0 °C
2.14 ft-lb/in²

@Temperature -4.00 °F
ISO 180/1A
Borealis Daplen™ EF005AE Polypropylene TPO Compound
Daplen™ EF005AE is a 10% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness, give..
Izod Impact, Notched (ISO) 4.50 kJ/m²

@Temperature -20.0 °C
2.14 ft-lb/in²

@Temperature -4.00 °F
ISO 180/1A
Borealis Daplen™ EF261AI Polypropylene TPO Compound
Daplen™ EF261AI is a 20 % mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and is easy to process...
Izod Impact, Notched (ISO) 4.50 kJ/m²

@Temperature 23.0 °C
2.14 ft-lb/in²

@Temperature 73.4 °F
ISO 180
Polyram PlusTek PB340S50 Nylon 6 for Injection Molding, 50% Glass-beads Reinforced, Heat Stabilized
50% Glass-beads reinforced, heat stabilized Nylon 6 for injection molding applications.Information provided by Polyram.
Izod Impact, Notched (ISO) 4.50 kJ/m²

@Temperature -20.0 °C
2.14 ft-lb/in²

@Temperature -4.00 °F
ISO 180
Total PPC 11750 Polypropylene, Heterophasic Copolymer, Injection Molding
Polypropylene PPC 11750 is a nucleated and controlled-rheology heterophasic copolymer with very high Melt Flow index of 50 g/10 min.Polypropylene PPC 11750 is characterized by good impact resistance..
Izod Impact, Notched (ISO) 4.50 kJ/m²

@Temperature 23.0 °C
2.14 ft-lb/in²

@Temperature 73.4 °F
ISO 180
Eastman Eastar EN001 Copolyester
Eastar EN001 Copolyester is a thermoplastic polyester copolymer. Eastar EN001 Copolyester has a relatively slow crystallization rate. This broadens the operating window for extrusion and forming pro..
Izod Impact, Notched (ISO) 4.50 kJ/m²

@Temperature 0.000 °C
2.14 ft-lb/in²

@Temperature 32.0 °F
ISO 180/1A
Domo 2348M Polypropylene Copolymer
Information provided by Domo.
Izod Impact, Notched (ISO) 4.50 kJ/m²

@Temperature 23.0 °C
2.14 ft-lb/in²

@Temperature 73.4 °F
DAM; ISO 180/1A
DuPont Performance Polymers Zytel® RS 3061HSL BK039A Nylon 610  (Unverified Data**)
Zytel® RS 3061HSL BK039A is a renewably sourced polyamide 610 resin containing a minimum of 60% renewably sourced ingredient by weight. It is an unreinforced, heat stabilized, lubricated black grad..
Izod Impact, Notched (ISO) 4.50 kJ/m²

@Temperature -40.0 °C
2.14 ft-lb/in²

@Temperature -40.0 °F
ISO 180
BASF Nypel® 2351 HS BK PA6 (Dry)
Description: Nypel® 2351 HS BK is a heat stabilized, pigmented black, impact modified PA6 extrusion grade compound. Quality and performance are combines at a lower cost. It is based on recycled PA6..
Izod Impact, Notched (ISO) 4.50 kJ/m²

@Temperature 23.0 °C
2.14 ft-lb/in²

@Temperature 73.4 °F
ISO 180
Eastman 9921W PET Injection Molded  (discontinued **)
Voridian PET 9921W is a copolymer PET. Typical applications include containers for automotive parts, household products, and pharmaceutical and food packaging. Voridian PET thermoplastic polyesters ..
Izod Impact, Notched (ISO) 4.50 kJ/m²

@Temperature 23.0 °C
2.14 ft-lb/in²

@Temperature 73.4 °F
50%RH; ISO 180/1A
DuPont Performance Polymers Zytel® SC315 NC010 Nylon 612  (Unverified Data**)
Zytel® SC315 NC010 is an unreinforced, lubricated 612 polyamide suitable for injection molding. It has been developed for applications such as parts for the healthcare industry.Information provided..
Izod Impact, Notched (ISO) 4.50 kJ/m²

@Temperature -30.0 °C
2.14 ft-lb/in²

@Temperature -22.0 °F
DAM; ISO 180/1A
DuPont Performance Polymers Zytel® SC315 NC010 Nylon 612  (Unverified Data**)
Zytel® SC315 NC010 is an unreinforced, lubricated 612 polyamide suitable for injection molding. It has been developed for applications such as parts for the healthcare industry.Information provided..
Izod Impact, Notched (ISO) 4.50 kJ/m²

@Temperature -30.0 °C
2.14 ft-lb/in²

@Temperature -22.0 °F
ISO 180/A
BASF Ultramid® B3UGM210 GR 22866 10/50% Glass/Mineral Filled PA6 FR (Dry)
Description: Halogen- and phosphorus-free injection-molding grade with very high rigidity, low smoke density and outstanding electrical properties.Information provided by BASF