Trade Name PPC
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total PPC 11750 Polypropylene, Heterophasic Copolymer, Injection Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polypropylene PPC 11750 is a nucleated and controlled-rheology heterophasic copolymer with very high Melt Flow index of 50 g/10 min.Polypropylene PPC 11750 is characterized by good impact resistance.Polypropylene PPC 10641 has been developed for high speed injection molding of thin walled packaging containers.Information provided by Total Petrochemicals.
Physical Properties Metric English Comments
Specific Gravity 0.905 g/cc
0.905 g/cc
ISO 1183
Bulk Density 0.525 g/cc
0.0190 lb/in³
ISO 1183
Melt Flow 50 g/10 min

@Load 2.16 kg,
Temperature 230 °C
50 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Rockwell R 83
83
ISO 2039-2
Tensile Strength, Yield 23.0 MPa
3340 psi
ISO 527-2
Elongation at Yield 4.5 %
4.5 %
ISO 527-2
Tensile Modulus 1.25 GPa
181 ksi
ISO 527-2
Flexural Modulus 1.20 GPa
174 ksi
ISO 178
Izod Impact, Notched (ISO) 4.50 kJ/m²

@Temperature -20.0 °C
2.14 ft-lb/in²

@Temperature -4.00 °F
ISO 180
8.00 kJ/m²

@Temperature 23.0 °C
3.81 ft-lb/in²

@Temperature 73.4 °F
ISO 180
Charpy Impact, Notched 0.450 J/cm²

@Temperature -20.0 °C
2.14 ft-lb/in²

@Temperature -4.00 °F
ISO 179
0.900 J/cm²

@Temperature 23.0 °C
4.28 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Thermal Properties Metric English Comments
Melting Point 165 °C
329 °F
ISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 100 °C
212 °F
120°C per hour; ISO 752
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C
131 °F
120°C per hour; ISO 752
Vicat Softening Point 70.0 °C

@Load 5.10 kg
158 °F

@Load 11.2 lb
50°C per hour; ISO 306
140 °C

@Load 1.02 kg
284 °F

@Load 2.25 lb
50°C per hour; ISO 306