Polymer Property : Tensile Strength at Break = 32600 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break >= 225 MPa

@Temperature 200 °C
>= 32600 psi

@Temperature 392 °F
PEAK Werkstoff DISPAL S541 Aluminum Alloy, AlMg6Mn4SiTiZr, Condition F
Information provided by PEAK Werkstoff GmbH
Tensile Strength at Break 225 MPa

@Temperature 23.0 °C
32600 psi

@Temperature 73.4 °F
LATI Laramid G/35 PPA, 35% Glass Fiber Reinforced
Semi-aromatic polyamide (PPA) based compound. Glass fibers. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; ..
Tensile Strength at Break 225 MPa

@Temperature 90.0 °C
32600 psi

@Temperature 194 °F
LATI Larpeek 10 K/30 PEEK, 30% Carbon Fiber Reinforced
Polyetheretherketone (PEEK) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As..
Tensile Strength at Break 225 MPa

@Temperature 23.0 °C
32600 psi

@Temperature 73.4 °F
LATI Larpeek 50 K/30 PEEK, 30% Carbon Fiber Reinforced
Polyetheretherketone (PEEK) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As..
Tensile Strength at Break 225 MPa

@Temperature 23.0 °C
32600 psi

@Temperature 73.4 °F
LATI Larpeek 10 G/60 PEEK, 60% Glass Fiber Reinforced
Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As..
Tensile Strength at Break 225 MPa

@Temperature 60.0 °C
32600 psi

@Temperature 140 °F
LATI Latigloss 57 G/50 F2 PPA, 50% Glass Fiber Reinforced
Product with high mechanical properties and exceptional surface finish based on Semi-aromatic polyamide (PPA). Glass fibers. Potentially suitable for food/medical contact application. Availability: ..
Tensile Strength at Break 225 MPa

@Temperature 23.0 °C
32600 psi

@Temperature 73.4 °F
3; ISO 527-2
Solvay Specialty Polymers Amodel® A-4145 HH Polyphthalamide (PPA), 45% Glass Fiber (Dry)
Amodel® A-4145 HH is a 45% glass fiber reinforced heat stabilized grade of polyphthalamide (PPA) that has been designed to provide outstanding property retention to thermal oxidative degradation ..
Tensile Strength at Break 225 MPa

@Temperature 23.0 °C
32600 psi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® 70G43HSLA BK099 Nylon 66  (Unverified Data**)
Zytel® 70G43HSLA BK099 is a 43% glass fiber reinforced, heat stabilized, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers