Material Notes:
Product Description: HD 6719 is a narrow molecular weight hexane copolymer designed for a wide rage of injection molding applications, combining easy processability with good toughness properties. Ideally suited for articles requiring low warpage, glossy surfaces and cold temperature impact resistance.Availability: Latin America, North America and South America Additive: Antioxidant: YesApplications: Food Packaging ContainersHouseware ArticlesLawn & Garden AccessoriesSoda Carrier TotesToys Information provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Density 0.952 g/cc
0.0344 lb/in³
ASTM D4883
Melt Flow 19 g/10 min

@Load 2.16 kg,
Temperature 190 °C
19 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 25.5 MPa
3700 psi
ASTM D638
Elongation at Break 270 %
270 %
ASTM D638
Flexural Modulus 1.10 GPa
160 ksi
2% Secant; ASTM D790
Flexural Modulus, 1% Secant 1240 MPa
180000 psi
ASTM D790
Izod Impact, Notched 0.326 J/cm

@Temperature -40.0 °C
0.610 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Thermal Properties Metric English Comments
Melting Point 132 °C
270 °F
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 67.0 °C
153 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 38.0 °C
100 °F
ASTM D648
Descriptive Properties Value Comments
Features Anti-static Agent
Form Pellet