Mechanical Properties Metric English Comments
K (wear) Factor 201 x 10-8 mm³/N-M
100 x 10-10 in³-min/ft-lb-hr
QTM 55010
Quadrant EPP Ketron® HPV PEEK High Pressure Velocity Polyetherether Ketone (ASTM Product Data Sheet)
This bearing grade of extruded Ketron PEEK offers the lowest coefficient of friction and best machinability of all Ketron grades. It is ideal for low wear, high PV parts that require chemical resis..
K (wear) Factor 201 x 10-8 mm³/N-M
100 x 10-10 in³-min/ft-lb-hr
QTM 55100
Quadrant EPP Nylatron® 4.6 (ASTM Product Data Sheet)
K (wear) Factor 201 x 10-8 mm³/N-M
100 x 10-10 in³-min/ft-lb-hr
QTM 55010
Quadrant EPP Nylatron® MC® 901 Blue, Heat Stabilized, Type 6 (ASTM Product Data Sheet)
Data provided by Quadrant Engineering Plastic ProductsBroadest size range availabilityGood mechanical and electrical propertiesIdeal balance of strength and toughnessCast as finished parts and near ..
K (wear) Factor 201 x 10-8 mm³/N-M
100 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP AL003 ABS
LNP LUBRICOMP* AL003 is a compound based on Acrylonitrile Butadiene Styrene resin containing 15% PTFE. Added features of this material include: Internally Lubricated.
K (wear) Factor 201 x 10-8 mm³/N-M
100 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP ZFL31XXC PPE+PS
LNP* LUBRICOMP* ZFL31XXC is a compound based on PPE+PS resin containing 5% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant
K (wear) Factor 201 x 10-8 mm³/N-M
100 x 10-10 in³-min/ft-lb-hr
Thrust washer at 2000 PV
Techmer ES Plaslube® AC-80/TF/15 Acetal (Copolymer), 15% PTFE
Plaslube polytetrafluoroethylene (PTFE) lubricated acetal copolymer grades offer additional wear and friction performance over neat acetal. Typical applications include bearings, slides and small g..
K (wear) Factor 201 x 10-8 mm³/N-M
100 x 10-10 in³-min/ft-lb-hr
Thrust washer at 2000 PV
Techmer ES Plaslube® NY-1/TF/10 Nylon 66, 10% PTFE
Plaslube polytetrafluoroethylene (PTFE) lubricated nylon 66 grades offer the best wear and friction properties of any unreinforced, lubricated nylon compounds, making them ideal materials for bearin..
K (wear) Factor 201 x 10-8 mm³/N-M
100 x 10-10 in³-min/ft-lb-hr
QTM 55010
Quadrant EPP Nylatron® MC® 907 Natural Nylon, Monocast® FDA Compliant, Unfilled Type 6 (ASTM Product Data Sheet)
K (wear) Factor 201 x 10-8 mm³/N-M
100 x 10-10 in³-min/ft-lb-hr
QTM 55010
Quadrant EPP Semitron® ESd 420- CM Dissipative Polyetherimide(ASTM Product Data Sheet)