Material Notes:
Plaslube polytetrafluoroethylene (PTFE) lubricated nylon 66 grades offer the best wear and friction properties of any unreinforced, lubricated nylon compounds, making them ideal materials for bearings and bushings.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ASTM D792
Water Absorption 0.70 %
0.70 %
24 hrs. ASTM D570
Linear Mold Shrinkage 0.015 cm/cm

@Thickness 3.17 mm
0.015 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 65.5 MPa
9500 psi
ASTM D638
Elongation at Break 4.5 %
4.5 %
ASTM D638
Flexural Yield Strength 89.6 MPa
13000 psi
ASTM D790
Flexural Modulus 2.90 GPa
420 ksi
ASTM D790
Izod Impact, Notched 0.427 J/cm

@Thickness 3.17 mm
0.800 ft-lb/in

@Thickness 0.125 in
ASTM D256
Coefficient of Friction, Dynamic 0.20
0.20
Coefficient of Friction, Static 0.12
0.12
K (wear) Factor 201 x 10-8 mm³/N-M
100 x 10-10 in³-min/ft-lb-hr
Thrust washer at 2000 PV
Limiting Pressure Velocity 0.420 MPa-m/sec
12000 psi-ft/min
at 100 FPM, ambient temperature, thrust washer.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 87.8 °C
190 °F
ASTM D648
Copyright © lookpolymers.com All Rights Reserved