Mechanical Properties Metric English Comments
Tensile Strength, Yield 280 MPa

@Strain 1.00 %,
Temperature 50.0 °C
40600 psi

@Strain 1.00 %,
Temperature 122 °F
EN min.; EN 10002-5
Outokumpu 153MA™ High Temperature Austenitic Stainless Steel
Variant of 1.4301 with increased silicon and nitrogen contents and microalloyed with rare earth metals (REM). This raises the max service temperature in dry air to 1000°C.Applications: Heat and cr..
Tensile Strength, Yield 280 MPa

@Strain 0.200 %,
Temperature 50.0 °C
40600 psi

@Strain 0.200 %,
Temperature 122 °F
EN min.; EN 10002-5
Outokumpu 253MA® High Temperature Austenitic Stainless Steel
Variant of 1.4828 with increased nitrogen content and has been microalloyed with rare earth metals (REM). The most suitable temperature range is 850-1100°C, because structural changes when used be..
Tensile Strength, Yield 280 MPa

@Strain 1.00 %
40600 psi

@Strain 1.00 %
Outokumpu Typical,Cold Rolled Narrow Strip; EN 10002-1
Outokumpu 4303 Cr-Ni Austenitic Stainless Steel
Good corrosion resistance with excellent drawing properties.Applications: Suitable for cold formed components where good workability is required. Fasteners, studs.Available in hot rolled plate (Qua..
Tensile Strength, Yield 280 MPa

@Strain 0.200 %
40600 psi

@Strain 0.200 %
Outokumpu Typical,Hot Rolled Plate (Quarto); EN 10002-1
Outokumpu 4306 Cr-Ni Austenitic Stainless Steel
General purpose steel with good corrosion resistance.Applications: Wide variety of applications in construction, chemical, petroleum, automobile, and domestic appliance markets.Available in hot roll..
Tensile Strength, Yield 280 MPa

@Strain 0.200 %
40600 psi

@Strain 0.200 %
Outokumpu Typical,Hot Rolled Plate (Quarto); EN 10002-1
Outokumpu 4307 Cr-Ni Austenitic Stainless Steel
General purpose steel with good corrosion resistance.Applications: Wide variety of applications in construction, chemical, petroleum, automobile, and domestic appliance markets.Available in hot roll..
Tensile Strength, Yield 280 MPa

@Strain 0.200 %
40600 psi

@Strain 0.200 %
Outokumpu Typical,Hot Rolled Plate (Quarto); EN 10002-1
Outokumpu 4401 Cr-Ni-Mo Austenitic Stainless Steel
General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r..
Tensile Strength, Yield 280 MPa

@Strain 0.200 %
40600 psi

@Strain 0.200 %
Outokumpu Typical,Hot Rolled Plate (Quarto); EN 10002-1
Outokumpu 4404 Cr-Ni-Mo Austenitic Stainless Steel
General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r..
Tensile Strength, Yield 280 MPa

@Strain 0.200 %
40600 psi

@Strain 0.200 %
EN min.,RT; EN 10002-1
Outokumpu 4406 Cr-Ni-Mo Austenitic Stainless Steel
Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and rod forms..
Tensile Strength, Yield 280 MPa

@Strain 0.200 %
40600 psi

@Strain 0.200 %
EN min.,RT; EN 10002-1
Outokumpu 4429 Cr-Ni-Mo Austenitic Stainless Steel
Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), cold rolled strip/sheet and rod forms.
Tensile Strength, Yield 280 MPa

@Strain 0.200 %
40600 psi

@Strain 0.200 %
Outokumpu Typical,Hot Rolled Plate (Quarto); EN 10002-1
Outokumpu 4432 Cr-Ni-Mo Austenitic Stainless Steel
General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r..
Tensile Strength, Yield 280 MPa

@Strain 0.200 %,
Temperature 200 °C
40600 psi

@Strain 0.200 %,
Temperature 392 °F
EN min.; EN 10002-5
Outokumpu SAF 2304® Duplex Stainless Steel
Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical tankersSeawater systemsFirewalls and blast walls on offshore platformsBridgesCompone..
Tensile Strength, Yield >= 280 MPa

@Strain 0.200 %
>= 40600 psi

@Strain 0.200 %
Industeel CLC 17.13.3 LN Nitrogen Containing 18Cr-10Ni-2Mo Austenitic Stainless Steel
Description: CLC 17-13-3LN is a nitrogen alloyed austenitic stainless steel with Mo additions. Its low carbon content avoids intergranular corrosion, even on welded pieces without an ulterior water ..
Tensile Strength, Yield 280 MPa

@Strain 0.200 %
40600 psi

@Strain 0.200 %
Typical
Industeel CLC 18.10Ti Titanium-Stabilized 18Cr-10Ni Austenitic Stainless Steel
CLC 18-10Ti is a 18Cr-9Ni austenitic stainless steel stabilized with some Titanium additions. This is a basic grades in the stainless steel range. Titanium bearing (carbide forming element) avoids i..
Tensile Strength, Yield 280 MPa

@Thickness 3.20 mm,
Temperature 427 °C
40600 psi

@Thickness 0.126 in,
Temperature 801 °F
0.2% Offset
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Sheet, Cold Rolled and Solution Annealed
HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing..
Tensile Strength, Yield >= 280 MPa

@Strain 0.200 %,
Thickness 152.4 - 203.2 mm
>= 40600 psi

@Strain 0.200 %,
Thickness 6.000 - 8.000 in
Tempers T851/T852
Constellium Alumold® 350 Aluminum
Alumold-350® has been specifically developed to achieve the best combination of strength at low and high temperatures, together with a good shape stability and machinability. Alumold-350® is parti..
Tensile Strength, Yield 280 - 450 MPa

@Thickness <=3.17 mm
40600 - 65300 psi

@Thickness <=0.125 in
transverse
American Utility Metals 3CR12® Stainless Steel
3CR12 is a weldable ferritic stainless steel, specifically designed for aggressive material handling applications. It is intended to provide the benefits of traditional stainless steel, such as stre..
Tensile Strength, Yield 280 MPa

@Strain 0.200 %,
Temperature 300 °C
40600 psi

@Strain 0.200 %,
Temperature 572 °F
Typical annealed sample; short time elevated temp.
American Utility Metals Cromgard® Stainless Steel
Cromgard is a low cost stainless steel, which is able to provide benefits of good weldability and formability, making it capable of fabrication by conventional techniques. It provides the benefits o..
Tensile Strength, Yield >= 280 MPa

@Strain 0.200 %,
Thickness >=7.938 mm
>= 40600 psi

@Strain 0.200 %,
Thickness >=0.3125 in
per ASTM A240; transverse; 0.2% Proof
American Utility Metals Cromgard® Stainless Steel
Cromgard is a low cost stainless steel, which is able to provide benefits of good weldability and formability, making it capable of fabrication by conventional techniques. It provides the benefits o..
Tensile Strength, Yield 280 MPa

@Thickness 3.20 mm,
Temperature 427 °C
40600 psi

@Thickness 0.126 in,
Temperature 801 °F
0.2% offset
Haynes Hastelloy® C-4 alloy, sheet, aged 100 hours at 899°C
Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) range. T..
Tensile Strength, Yield >= 280 MPa

@Strain 0.200 %
>= 40600 psi

@Strain 0.200 %
Industeel URANUS® S1 4 % Si, Austenitic Stainless Steel Resistant to Nitric Acid Solutions
Description: Research carried out in about the last fifteen years in CREUSOT LOIRE INDUSTRIE laboratories shows that a strong addition of silicon to austenitic stainless steels of the 18/10 type has..