Polymer Property : Tensile Strength, Yield = 10.8 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 7.20 - 10.8 MPa
1040 - 1570 psi
±20% change after 168 hours @ 70°C; ASTM D412
Precision Polymer Engineering S50K Silicone Rubber
Silicone Rubber, 45-55 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. Formulated using only those ingredients determined by the United States Federal..
Tensile Strength, Yield 7.20 - 10.8 MPa
1040 - 1570 psi
±20% change after 168 hours @ 70°C; ASTM D412
Precision Polymer Engineering S60K Silicone Rubber
Silicone Rubber, 56-65 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. Formulated using only those ingredients determined by the United States Federal..
Tensile Strength, Yield 7.20 - 10.8 MPa
1040 - 1570 psi
±20% change after 168 hours @ 70°C; ASTM D412
Precision Polymer Engineering S70H Silicone Rubber
White Silicone Rubber, 68-78 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. Formulated using only those ingredients determined by the United States F..
Tensile Strength, Yield 4.00 - 10.8 MPa
580 - 1570 psi
Average value: 7.34 MPa Grade Count:21
Overview of materials for Ethylene Acrylic Acid
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Acrylic Acid". Each property range of values reported is minimum and maximum values of appropri..