Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 4.00 MPa | 580 psi | ISO 527 |
Polimeri Europa Greenflex® MQ 40 Ethylene Vinyl Acetate Copolymer - Injection Molding & Compounding Greenflex MQ 40 is an ethylene vinyl acetate copolymer (EVA) for injection molding and compounding applications. Greenflex MQ 40 combines high fluidity and high elasticity.Main Applications: Green.. |
|||
Tensile Strength, Yield | 4.00 MPa | 580 psi | chs 20 in/min; ASTM D412 |
Network Polymers Softflex® 0350 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
Tensile Strength, Yield | 4.00 - 10.8 MPa | 580 - 1570 psi | Average value: 7.34 MPa Grade Count:21 |
Overview of materials for Ethylene Acrylic Acid This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Acrylic Acid". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Tensile Strength, Yield | 4.00 MPa | 580 psi | 150°C for 1,000 hrs |
Fujipoly Industries Sarcon® 85U Thin-Film UR Sarcon UR is Fujipolys originally developed High Heat Conductive/Low Hardness Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Information prov.. |
|||
Tensile Strength, Yield | 4.00 MPa | 580 psi | Support Rubber |
Fujipoly Industries Zebra® Silver Connector Fujipoly New High performance Silver Zebra connectors are constructed of alternating parallel layers of electrically conductive and nonconductive silicone elastomer. The electrically conductive laye.. |
|||
Tensile Strength, Yield | 4.00 MPa | 580 psi | 50 mm/min; ISO 527-1/-2 |
Styrolution Styroflex® 2G 66 SBC Description: Styroflex® 2G 66 is a styrene-butadiene block copolymer (SBC) with the properties of a thermoplastic elastomer (S-TPE). Styroflex® 2G 66 is the only S-TPE with a styrene content o.. |
|||
Tensile Strength, Yield | 4.00 MPa | 580 psi | 100%; ASTM D412 |
Teknor Apex APEX® 3210-65 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, Radiation Uses-Automotive Applications, Connectors, Non-specific Food Applications, Ge.. |
|||
Tensile Strength, Yield | 4.00 MPa | 580 psi | ASTM D638 |
A. Schulman POLYFORT™ PX 1042 Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 4.00 MPa | 580 psi | ASTM D638 |
A. Schulman POLYFORT™ PX 1042 Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 4.00 MPa | 580 psi | Elastic Limit |
Wolf Kunststoff ZEDEX® ZX-100EL55 A1F Polymer Alloy, Elastomer Modified Main Characteristics: Rubbery; Soft; High shock absorption; High impact resistance; Elongation > 300%Applications: Handling, Vessel and Pump, Steel and Water, Chemical Engineering, Automitve Technol.. |
|||
Tensile Strength, Yield | 4.00 MPa | 580 psi | |
Trelleborg B500 Commercial Nitrile Rubber Nitrile rubber or acrylonitrile-butadiene rubber is a copolymer of butadiene and acrylonitrile.PropertiesGood general resistance to oils.Good mechanical properties especially tensile strength, flexi.. |
|||
Tensile Strength, Yield | 4.00 MPa | 580 psi | |
Trelleborg B700 Commercial Nitrile Rubber Nitrile rubber or acrylonitrile-butadiene rubber is a copolymer of butadiene and acrylonitrile.PropertiesGood general resistance to oils.Good mechanical properties especially tensile strength, flexi.. |
|||
Tensile Strength, Yield | 4.00 MPa | 580 psi | |
Trelleborg Commercial Neoprene® C798 Chloroprene CR or Chloroprene is a homopolymer of chloroprene or chlorobutadiene. NEOPRENE®PropertiesExcellent mechanical and abrasion properties even without reinforcing fillers.Reasonable resilience in grade.. |
|||
Tensile Strength, Yield | 4.00 MPa | 580 psi | |
Trelleborg Z800 Commercial SBR Rubber Styrene-butadiene Rubber is a co-polymer of styrene and butadiene.PropertiesIts general properties are similar to those of natural rubber, but it is more resistant to aging and temperature, and like.. |
|||
Tensile Strength, Yield | 4.00 MPa | 580 psi | ASTM D638 |
A. Schulman POLYFORT™ PX 1042 Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 4.00 MPa | 580 psi | 2" (50mm) per min; ASTM D638 |
Formosa Plastics Formolene® 5143S Homopolymer Polypropylene Homopolymer for Extrusion Sheet and Thermoforming Applications Formolene® 5143S is a higher melt flow homopolymer designed for light weighting of components. Its very high stiffness enables reducti.. |
|||
Tensile Strength, Yield | 4.00 MPa | 580 psi | |
Trelleborg B600 Commercial Nitrile Rubber Nitrile rubber or acrylonitrile-butadiene rubber is a copolymer of butadiene and acrylonitrile.PropertiesGood general resistance to oils.Good mechanical properties especially tensile strength, flexi.. |
|||
Tensile Strength, Yield | 4.00 MPa | 580 psi | ASTM D638 |
A. Schulman POLYFORT™ PX 1042 Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 4.00 MPa @Strain 50.0 % |
580 psi @Strain 50.0 % |
50 mm/min |
Arkema Group Nakan® FMM 611 N PVC, Soft Injection Molding Grade NAKAN FMM 611 N is a soft polyvinyl chloride compound developed for injection molding of breathing masks and general purpose.ISO data provided by the manufacturer, Arkema. |
|||
Tensile Strength, Yield | 4.00 MPa | 580 psi | |
ACC MM239 Addition Cure 2-Part Molding Rubber Part of the Amber Chemical Group. Data provided by manufacturer.Characteristics: cures at room temperature, low shrinkage, high tear and tensile strengths. Applications: ceramic/polyester/PU/epoxy a.. |
|||
Tensile Strength, Yield | 4.00 MPa | 580 psi | 50 mm/min |
Arkema Group Evatane® 1005 VN 5 Ethylene Vinyl Acetate EVA copolymer made by high pressure tubular process. Applications Grade for films with high transparency and high mechanical properties. Examples: coextrusion, stretch film, paper-stationary, fancy .. |
|||
Tensile Strength, Yield | 4.00 - 8.00 MPa | 580 - 1160 psi | Average value: 5.67 MPa Grade Count:3 |
Overview of materials for Very Low Density Polyethylene (VLDPE) This property data is a summary of similar materials in the MatWeb database for the category "Very Low Density Polyethylene (VLDPE)". Each property range of values reported is minimum and maximum va.. |
|||
Tensile Strength, Yield | 4.00 MPa | 580 psi | |
Trelleborg Commercial Neoprene® C400 Chloroprene CR or Chloroprene is a homopolymer of chloroprene or chlorobutadiene. NEOPRENE®PropertiesExcellent mechanical and abrasion properties even without reinforcing fillers.Reasonable resilience in grade.. |
|||
Tensile Strength, Yield | 4.00 MPa | 580 psi | |
Trelleborg Z600 Commercial SBR Rubber Styrene-butadiene Rubber is a co-polymer of styrene and butadiene.PropertiesIts general properties are similar to those of natural rubber, but it is more resistant to aging and temperature, and like.. |
|||
Tensile Strength, Yield | 4.00 MPa @Strain 300 % |
580 psi @Strain 300 % |
Method A (Dumbbell & Section), 20 in/min; ASTM D412 |
PolyOne Synprene® IT 37-023 Thermoplastic Elastomer - SBC, Mineral Filled
(discontinued **) Description/Features:Multi-Purpose Thermoplastic ElastomerMineral FilledApplications:General PurposeMarket:Consumer GoodsIndustrialProcessing Method:Injection MoldingPolyOne First ChoiceInformation .. |
|||
Tensile Strength, Yield | 4.00 MPa | 580 psi | ASTM D638 |
A. Schulman POLYFORT™ PX 1042 Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 4.00 MPa | 580 psi | ISO 527 |
Breplast Bretene SP Polypropylene / Polyethylene Composite Recovered polypropylene and polyethylene compositeInformation provided by Breplast S.p.A. |
|||
Tensile Strength, Yield | 4.00 MPa | 580 psi | ISO 527 |
Lucobit Lucofin® 1400HN Ethylene Butyl Acrylate Lucofin 1400HN is a polar copolymer consisting of ethylene and butyl acrylate with low crystallinity. Due to its chemical structure Lucofin 1400HN is softer and more flexible than ethylene homopolym.. |
|||
Tensile Strength, Yield | 4.00 MPa | 580 psi | Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412 |
PolyOne Synprene® RT-3740 Thermoplastic Elastomer - SBC, Mineral Filled
(discontinued **) Description/Features:Multi-Purpose Thermoplastic ElastomerMineral FilledNaturalApplications:General PurposeMarket:Consumer GoodsIndustrialBuilding and ConstructionProcessing Method:Injection Molding.. |
|||
Tensile Strength, Yield | 4.00 MPa @Strain 50.0 % |
580 psi @Strain 50.0 % |
50 mm/min |
Arkema Group Nakan® FMS 601 L PVC, Soft Injection Molding Grade NAKAN FMS 601 L is a soft polyvinyl chloride compound developed for injection molding of various applications for automotive ( handles, hand grasps, etc...)ISO data provided by the manufacturer, Ark.. |