Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Yield = 110 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 96.5 - 110 MPa
14000 - 16000 psi
Average value: 105 MPa Grade Count:4
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 20% Carbon Fiber Filled". Specific grades with carbon fiber conte..
Tensile Strength, Yield 81.4 - 110 MPa
11800 - 16000 psi
Average value: 94.0 MPa Grade Count:7
Overview of materials for Nylon 66, Aramid Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Aramid Fiber Filled". Each property range of values reported is minimum and maximum values of ..
Tensile Strength, Yield 75.0 - 110 MPa
10900 - 16000 psi
Average value: 93.5 MPa Grade Count:6
Overview of materials for Polyphenylene Ether, Glass/Graphite Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Glass/Graphite Reinforced". Each property range of values reported is minimum and m..
Tensile Strength, Yield 60.0 - 110 MPa
8700 - 16000 psi
Average value: 82.7 MPa Grade Count:13
Overview of materials for Nylon 6, MoS2 Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropria..
Tensile Strength, Yield 50.0 - 110 MPa
7250 - 16000 psi
Average value: 82.9 MPa Grade Count:6
Overview of materials for Polystyrene + Polyphenylene Ether, Glass Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Glass Filler". Each property range of values reported is minimum and ..
Tensile Strength, Yield 36.0 - 110 MPa
5220 - 16000 psi
Average value: 76.5 MPa Grade Count:111
Overview of materials for Polypropylene with 30% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Glass Fiber Filler". Specific grades with glass content between 25% and 34% are i..
Tensile Strength, Yield 8.96 - 110 MPa
1300 - 16000 psi
Average value: 26.4 MPa Grade Count:712
Overview of materials for Polypropylene Copolymer
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene Copolymer". Each property range of values reported is minimum and maximum values of approp..