Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 96.5 - 110 MPa | 14000 - 16000 psi | Average value: 105 MPa Grade Count:4 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 20% Carbon Fiber Filled". Specific grades with carbon fiber conte.. |
|||
Tensile Strength, Yield | 81.4 - 110 MPa | 11800 - 16000 psi | Average value: 94.0 MPa Grade Count:7 |
Overview of materials for Nylon 66, Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Aramid Fiber Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Tensile Strength, Yield | 75.0 - 110 MPa | 10900 - 16000 psi | Average value: 93.5 MPa Grade Count:6 |
Overview of materials for Polyphenylene Ether, Glass/Graphite Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Glass/Graphite Reinforced". Each property range of values reported is minimum and m.. |
|||
Tensile Strength, Yield | 60.0 - 110 MPa | 8700 - 16000 psi | Average value: 82.7 MPa Grade Count:13 |
Overview of materials for Nylon 6, MoS2 Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropria.. |
|||
Tensile Strength, Yield | 50.0 - 110 MPa | 7250 - 16000 psi | Average value: 82.9 MPa Grade Count:6 |
Overview of materials for Polystyrene + Polyphenylene Ether, Glass Filler This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Glass Filler". Each property range of values reported is minimum and .. |
|||
Tensile Strength, Yield | 36.0 - 110 MPa | 5220 - 16000 psi | Average value: 76.5 MPa Grade Count:111 |
Overview of materials for Polypropylene with 30% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Glass Fiber Filler". Specific grades with glass content between 25% and 34% are i.. |
|||
Tensile Strength, Yield | 8.96 - 110 MPa | 1300 - 16000 psi | Average value: 26.4 MPa Grade Count:712 |
Overview of materials for Polypropylene Copolymer This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene Copolymer". Each property range of values reported is minimum and maximum values of approp.. |