Polymer Property : Tensile Strength, Yield = 1250 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 1180 - 1250 MPa
171000 - 181000 psi
Plansee DENAL® 920 60 20 Tungsten-Nickel-Iron-Cobalt Alloy
Characteristics:exceptionally stronghigh densityoutstanding mechanical damping capabilitiesHigh absorption of X-ray and gamma radiationInformation provided by Plansee.
Tensile Strength, Yield 1030 - 1250 MPa
149000 - 181000 psi
Materion Beryllium Copper Alloy 190 Strip; XHMS (TM08) Temper (UNS C17200)
Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 98%Stress Relaxation after 1000 hrs @ 200°C: 69%Formability Ratio, 90° Bend, R..
Tensile Strength, Yield 890 - 1250 MPa
129000 - 181000 psi
Materion Beryllium Copper Alloy 25 Plate & Rolled Bar; HT (TH04) Temper; over 51 to 76 mm Thickness (UNS C17200)
Treatment required for max strength: 2 hrs @ 330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In..
Tensile Strength, Yield 990 - 1250 MPa
144000 - 181000 psi
Materion Beryllium Copper Alloy 25 Wire; AT (TF00) Temper; 1.3-12.7 mm Diameter (UNS C17200)
Treatment required for max strength: 3 hrs @ 315-330°C Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed i..
Tensile Strength, Yield 990 - 1250 MPa
144000 - 181000 psi
Materion Beryllium Copper Alloy M25 Wire; AT (TF00) Temper; 1.3-12.7 mm Diameter (UNS C17300)
Treatment required for max strength: 3 hrs @ 315-330°C Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed i..
Tensile Strength, Yield 1100 - 1250 MPa
160000 - 181000 psi
Solution Annealed & Aged
Materion Beryllium Nickel M220C
Information supplied by Brush Wellman Engineered Materials.Brush M220C is characterized by high levels of strength, hardness, and thermal conductivity combined with excellent resistance to wear, cor..
Tensile Strength, Yield 950 - 1250 MPa

@Strain 0.200 %
138000 - 181000 psi

@Strain 0.200 %
SSAB Tunnplat Docol® 1200 DP High-strength Steel
The steels are annealed at temperatures between 750°C and 850°C, depending on the grade of steel, and then are hardened by quenching in water. Tempering is the next stage, in which the steel ..