Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lubrizol Estane® ALR E80A Thermoplastic Polyurethane

Category Polymer , Thermoplastic , Polyurethane, TP
Manufacturer Lubrizol (former Noveon)
Trade Name ESTANE®
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Lubrizol Estane® ALR E80A Thermoplastic Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Type: Estane® ALR E80A is a clear aliphatic thermoplastic polyurethane (TPU).Features: Non-yellowing with good mechanical properties.Information Provided by The Lubrizol Corporation
Physical Properties Metric English Comments
Specific Gravity 1.05 g/cc
1.05 g/cc
ASTM D792
Linear Mold Shrinkage 0.0080 - 0.012 cm/cm
0.0080 - 0.012 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore A 77
77
ASTM D2240
Tensile Strength, Ultimate 42.7 MPa
6200 psi
ASTM D412
Tensile Strength, Yield 4.14 MPa
600 psi
at 100%; ASTM D412
6.21 MPa
900 psi
at 200%; ASTM D412
9.65 MPa
1400 psi
at 300%; ASTM D412
Elongation at Break 550 %
550 %
ASTM D412
Flexural Modulus 0.0159 GPa
2.30 ksi
ASTM D790
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved