Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Yield = 117 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 42.0 - 117 MPa
6090 - 17000 psi
Average value: 79.2 MPa Grade Count:14
Overview of materials for Acetal Copolymer, 20% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% ar..
Tensile Strength, Yield 51.7 - 117 MPa
7500 - 17000 psi
Average value: 85.9 MPa Grade Count:32
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled". Specific grades with glass content betwe..
Tensile Strength, Yield 21.4 - 117 MPa
3100 - 17000 psi
Average value: 51.5 MPa Grade Count:20
Overview of materials for ABS/Polyester Alloy
This property data is a summary of similar materials in the MatWeb database for the category "ABS/Polyester Alloy". Each property range of values reported is minimum and maximum values of appropriat..
Tensile Strength, Yield 55.2 - 117 MPa
8000 - 17000 psi
0.2% offset
Eagle Brass 220 Commercial Bronze, Annealed
CDA 220 is known for having very good corrosion resistance, great cold workability and good hot workability for drawing, blanking, coining, stamping, piercing and punching. Typical uses include plum..
Tensile Strength, Yield 0.539 - 117 MPa
78.2 - 17000 psi
Average value: 61.4 MPa Grade Count:12
Overview of materials for Polycarbonate, Glass + PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass + PTFE Filled". Each property range of values reported is minimum and maximum value..
Tensile Strength, Yield 110 - 117 MPa
15900 - 17000 psi
Average value: 114 MPa Grade Count:4
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled". Each property range of values reported is ..
Tensile Strength, Yield 12.0 - 117 MPa

@Temperature -40.0 - 120 °C
1740 - 17000 psi

@Temperature -40.0 - 248 °F
Average value: 56.9 MPa Grade Count:8
Overview of materials for Nylon 6, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Impact Grade". Each property range of values reported is minimum and maximum values of appropri..
Copyright © lookpolymers.com All Rights Reserved