Mechanical Properties Metric English Comments
Tensile Strength, Yield 30.0 - 40.0 MPa
4350 - 5800 psi
Injection and Compression; ISO 527
Raschig Group 4552 Silicone
Glass fiber reinforced silicone molding compound. Excellent thermal stability - up to +/- 300°C continuously, excellent electrical properties, good mechanical strength, very good dimensional stabi..
Tensile Strength, Yield 1.38 - 40.0 MPa
200 - 5800 psi
Average value: 14.8 MPa Grade Count:50
Overview of materials for Epoxy Adhesive
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Adhesive". Each property range of values reported is minimum and maximum values of appropriate Mat..
Tensile Strength, Yield 0.130 - 40.0 MPa
18.9 - 5800 psi
Average value: 18.4 MPa Grade Count:80
Overview of materials for High Density Polyethylene (HDPE), Ultra High Molecular Weight
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Ultra High Molecular Weight". Each property range of values reported i..
Tensile Strength, Yield 40.0 - 40.0 MPa

@Temperature 90.0 - 140 °C
5800 - 5800 psi

@Temperature 194 - 284 °F
Average value: 40.0 MPa Grade Count:1
Overview of materials for Nylon 66/6
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6". Each property range of values reported is minimum and maximum values of appropriate MatWeb ..
Tensile Strength, Yield 40.0 - 40.0 MPa

@Time 1.80e+7 - 7.20e+7 sec
5800 - 5800 psi

@Time 5000 - 20000 hour
Average value: 40.0 MPa Grade Count:1
Overview of materials for Nylon 66/6
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6". Each property range of values reported is minimum and maximum values of appropriate MatWeb ..
Tensile Strength, Yield 34.0 - 40.0 MPa

@Thickness 2.00 mm
4930 - 5800 psi

@Thickness 0.0787 in
50 mm/min; ASTM D638
Solvay Specialty Polymers Solef® 60512 Polyvinylidene Fluoride (PVDF)
Solef® 60512 PVDF copolymer has high viscosity of the melt and it is a grade for offshore piping.Features: Copolymer; High ViscosityUses: PipingAdditional Properties: Crystallization Heat - ASTM ..
Tensile Strength, Yield 30.0 - 40.0 MPa

@Thickness 1.50 mm
4350 - 5800 psi

@Thickness 0.0591 in
50 mm/min; ASTM D638
Solvay Specialty Polymers Solef® 60512/0550 and 60512/0150 Polyvinylidene Fluoride (PVDF)
Solef® 60512/0550 and Solef® 60512/0150 are PVDF grades compounded with PTFE for extrusion of anti-wear tapes.Features: CopolymerUses: TapeAdditional Properties: Crystallization Heat - ASTM D3..
Tensile Strength, Yield 34.0 - 40.0 MPa

@Thickness 2.00 mm,
Temperature 23.0 °C
4930 - 5800 psi

@Thickness 0.0787 in,
Temperature 73.4 °F
Type IV, 50 mm/min; ASTM D638
Solvay Specialty Polymers Solef® 60512 Polyvinylidene Fluoride (PVDF)  (Unverified Data**)
Solef® 60512 PVDF copolymer has high viscosity of the melt and it is a grade for offshore piping.Information provided by Solvay Specialty Polymers.
Tensile Strength, Yield 21.0 - 40.0 MPa
3050 - 5800 psi
Average value: 28.4 MPa Grade Count:9
Overview of materials for Polypropylene, Wood Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Wood Filled". Each property range of values reported is minimum and maximum values of app..
Tensile Strength, Yield 0.110 - 40.0 MPa
16.0 - 5800 psi
Average value: 12.9 MPa Grade Count:484
Overview of materials for Thermoset Polyurethane, Elastomer, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Elastomer, Unreinforced". Each property range of values reported is minimum and ..