Mechanical Properties Metric English Comments
Tensile Strength, Yield 393 - 476 MPa
57000 - 69000 psi
0.2% offset
Eagle Brass 230 Red Brass, Hard
CDA 230 is known for having an electrical conductivity of 37% IACS, red color, corrosion resistance, excellent formability and moderate strength. Typical uses include costume jewelry, eyelets, faste..
Tensile Strength, Yield 379 - 476 MPa
55000 - 69000 psi
0.2% offset
Eagle Brass 260 Cartridge Brass, 3/4 Hard
Alloy C260 is commonly used for electrical components, electronic parts, and mechanical fasteners. The alloy has good strength but poor stress relaxation characteristics and does not make a particul..
Tensile Strength, Yield 172 - 476 MPa
25000 - 69000 psi
0.2% offset
Eagle Brass 715 Copper Nickel 30%, 1/4 Hard
715 exhibits excellent corrosion resistance, especially in marine applications. It has moderately high strength and has good creep resistance at elevated temperatures. The cost is relatively high co..
Tensile Strength, Yield 338 - 476 MPa
49000 - 69000 psi
0.2% offset
Eagle Brass 735 Nickel Silver 18%, 1/2 Hard
735 is used for coinage, name plates, zippers, flatware, and fashion jewelry.Information provided by Eagle Brass Company