Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 393 - 476 MPa | 57000 - 69000 psi | 0.2% offset |
Eagle Brass 230 Red Brass, Hard CDA 230 is known for having an electrical conductivity of 37% IACS, red color, corrosion resistance, excellent formability and moderate strength. Typical uses include costume jewelry, eyelets, faste.. |
|||
Tensile Strength, Yield | 379 - 476 MPa | 55000 - 69000 psi | 0.2% offset |
Eagle Brass 260 Cartridge Brass, 3/4 Hard Alloy C260 is commonly used for electrical components, electronic parts, and mechanical fasteners. The alloy has good strength but poor stress relaxation characteristics and does not make a particul.. |
|||
Tensile Strength, Yield | 172 - 476 MPa | 25000 - 69000 psi | 0.2% offset |
Eagle Brass 715 Copper Nickel 30%, 1/4 Hard 715 exhibits excellent corrosion resistance, especially in marine applications. It has moderately high strength and has good creep resistance at elevated temperatures. The cost is relatively high co.. |
|||
Tensile Strength, Yield | 338 - 476 MPa | 49000 - 69000 psi | 0.2% offset |
Eagle Brass 735 Nickel Silver 18%, 1/2 Hard 735 is used for coinage, name plates, zippers, flatware, and fashion jewelry.Information provided by Eagle Brass Company |