Polymer Property : Tensile Strength, Yield = 555 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 400 - 555 MPa

@Strain 0.200 %
58000 - 80500 psi

@Strain 0.200 %
ALIMEX AMP 8000 Aluminum Plate
AMP 8000 offers higher strength levels, good machinability and dimensional stability. Its tensile strength is up to 40% higher than AlZn5.5MgCu (7075). Moulding, (Prototypes) injection moulds, Jig ..