Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 400 - 555 MPa @Strain 0.200 % |
58000 - 80500 psi @Strain 0.200 % |
|
ALIMEX AMP 8000 Aluminum Plate AMP 8000 offers higher strength levels, good machinability and dimensional stability. Its tensile strength is up to 40% higher than AlZn5.5MgCu (7075). Moulding, (Prototypes) injection moulds, Jig .. |