Material Notes:
Type GE-30 combines improved strength and solidity with higher machining feeds and speeds than ordinary gray iron.General Meehanite information - Meehanite metal is first melted to a definite degree of undercooling or constitution which is related to the section of the casting to be poured and the range of physical properties such as tensile strength and hardness required. Nucleation with patented mixtures of graphitizing agents results in the removal of undercooling, in the controlled precipitation of graphite and in a fine grained eutectic cell structure which determines the density and physical integrity of the casting. Ordinary cast irons made to chemical specifications which do not include the benefit of controlled undercooling are influenced by mass effect to a maximum degree and for this and other reasons cannot be considered an equivalent to Meehanite metal.Information provided by Meehanite Marketing Association.
Physical Properties Metric English Comments
Specific Gravity 7.06 g/cc
7.06 g/cc
Mechanical Properties Metric English Comments
Hardness, Brinell <= 160
<= 160
Nominal
Tensile Strength, Ultimate 207 MPa
30000 psi
Tensile Strength, Yield 79.3 MPa
11500 psi
.01% permanent set
Modulus of Elasticity 89.6 GPa
13000 ksi
Modulus of Rupture 0.421 GPa
61.0 ksi
Compressive Strength 827 MPa
120000 psi
Poissons Ratio 0.27
0.27
Fatigue Strength 93.1 MPa
13500 psi
Machinability 38 %
38 %
Dalcher
Shear Modulus 38.3 GPa
5550 ksi
Shear Strength 207 MPa
30000 psi
Izod Impact Unnotched 8.13 - 16.3 J

@Diameter 20.3 mm
6.00 - 12.0 ft-lb

@Diameter 0.798 in
Thermal Properties Metric English Comments
CTE, linear 12.4 µm/m-°C

@Temperature 37.8 - 538 °C
6.90 µin/in-°F

@Temperature 100 - 1000 °F
Thermal Conductivity 41.8 W/m-K

@Temperature 10.0 - 232 °C
290 BTU-in/hr-ft²-°F

@Temperature 50.0 - 450 °F
Shrinkage 0.80 - 1.0 %
0.80 - 1.0 %
Patternmaker Shrinkage