Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.320 GPa | 46.4 ksi | ASTM D638 |
Aclo Accucomp Polyethylene LD0109L Low Density |
|||
Tensile Modulus | 0.320 GPa | 46.4 ksi | 1 mm/min |
Arkema Group Rilsan® BESN P40 TL Nylon 11, Flexible Tubing Grade (Conditioned) Designation ISO 1874-PA11-P,EHL,22-003Flexible grade for tubes extrusion. Available color: black and natural. Light and heat stabilized.High flexibility. High impact strength. Very good chemical res.. |
|||
Tensile Modulus | 0.320 GPa @Temperature 120 °C |
46.4 ksi @Temperature 248 °F |
ISO Data |
BASF Ultramid® 8202 HS PA6 (Conditioned) Ultramid 8202 HS is a heat stabilized, low viscosity, general purpose nylon 6 injection molding homopolymer. It possesses the combination of strength and toughness and has excellent chemical and ab.. |
|||
Tensile Modulus | 0.320 GPa @Temperature 120 °C |
46.4 ksi @Temperature 248 °F |
ISO Data |
BASF Ultramid® 8202 PA6 (Conditioned) Ultramid 8202 is a low viscosity, general purpose polyamide 6 injection molding homopolymer exhibiting excellent melt fluidity for filling thin sections. It is also available in heat stabilized (Ult.. |