Mechanical Properties Metric English Comments
Tensile Modulus 0.320 GPa
46.4 ksi
ASTM D638
Aclo Accucomp Polyethylene LD0109L Low Density
Tensile Modulus 0.320 GPa
46.4 ksi
1 mm/min
Arkema Group Rilsan® BESN P40 TL Nylon 11, Flexible Tubing Grade (Conditioned)
Designation ISO 1874-PA11-P,EHL,22-003Flexible grade for tubes extrusion. Available color: black and natural. Light and heat stabilized.High flexibility. High impact strength. Very good chemical res..
Tensile Modulus 0.320 GPa

@Temperature 120 °C
46.4 ksi

@Temperature 248 °F
ISO Data
BASF Ultramid® 8202 HS PA6 (Conditioned)
Ultramid 8202 HS is a heat stabilized, low viscosity, general purpose nylon 6 injection molding homopolymer. It possesses the combination of strength and toughness and has excellent chemical and ab..
Tensile Modulus 0.320 GPa

@Temperature 120 °C
46.4 ksi

@Temperature 248 °F
ISO Data
BASF Ultramid® 8202 PA6 (Conditioned)
Ultramid 8202 is a low viscosity, general purpose polyamide 6 injection molding homopolymer exhibiting excellent melt fluidity for filling thin sections. It is also available in heat stabilized (Ult..