Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 1.25 GPa | 181 ksi | ISO 527 |
Polikim Polypropylene Polypropylene is an olefin class plastic with low density. It has good chemical and electrical properties and is rigid. Its use under 0°C is not recommended as its mechanical properties weaken. Nor.. |
|||
Tensile Modulus | 1.25 GPa | 181 ksi | |
Radici Radilon® S 35HR (cond.) Nylon 6 PA6 medium-high viscosity injection molding grade. Easy mould release.Information provided by Radici group. |
|||
Tensile Modulus | 1.25 GPa | 181 ksi | |
Hybrid Plastics CO6U50.02 Nanoreinforced® Cyclic Olefin Copolymer Impact modified, flame retardantThe exceptional heat distortion temperature and low density of cyclic olefin copolymers (COC) makes them excellent materials for high temperature applications where l.. |
|||
Tensile Modulus | 1.25 GPa | 181 ksi | ISO 527 |
Iran Petrochemical (PCC) BL3 HF 4760 High Density Polyethylene BL3 is a high density polyethylene with 1-Butene as co monomer. It is high density and stiffness, good ESCR, high rigidity, good flowability and impact strength.Applications: small blow molding, bo.. |
|||
Tensile Modulus | 1.25 - 1.40 GPa @Thickness 2.00 mm |
181 - 203 ksi @Thickness 0.0787 in |
1.0 mm/min; ASTM D638 |
Solvay Specialty Polymers Solef® 60512 Polyvinylidene Fluoride (PVDF) Solef® 60512 PVDF copolymer has high viscosity of the melt and it is a grade for offshore piping.Features: Copolymer; High ViscosityUses: PipingAdditional Properties: Crystallization Heat - ASTM .. |
|||
Tensile Modulus | 1.25 GPa | 181 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON MD000 PP LNP STAT-KON* MD000 is a compound based on Polypropylene resin containing Carbon Powder. Added feature of this material is: Electrically Conductive. |
|||
Tensile Modulus | 1.25 GPa | 181 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON MD000 PP (Asia Pacific) LNP STAT-KON* MD000 is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive. |
|||
Tensile Modulus | 1.25 GPa | 181 ksi | 1mm/min; ISO 527-2 |
Borealis BC545MO Polypropylene Copolymer BC545MO is a low-blush polypropylene heterophasic copolymer intended for injection molding. This grade features high impact strength, high thermal stability and very good process ability. As all pol.. |
|||
Tensile Modulus | 1.25 GPa | 181 ksi | 1mm/min; ISO 527-2 |
Borealis BE170MO Polypropylene Copolymer BE170MO is a heterophasic copolymer. This grade is characterized by high impact strength, high stiffness and good flow properties. This grade contains additives providing low taste and odor as well.. |
|||
Tensile Modulus | 1.25 GPa | 181 ksi | 1mm/min; ISO 527-2 |
Borealis BL2571 High Density Polyethylene BL2571 is a high-density polyethylene with high stiffness and high environmental stress crack resistance. This product is intended for blow molding. Applications: household and chemical containers.. |
|||
Tensile Modulus | 1.25 GPa | 181 ksi | At 1 mm/min; ISO 527-2 |
Borealis Bormed™ BE860MO Polypropylene Copolymer for Healthcare Applications Bormed BE860MO is a heterophasic copolymer characterized by an excellent impact strength also at low temperatures (deep freeze applications) together with high stiffness and good flow properties.Bor.. |
|||
Tensile Modulus | 1.25 GPa | 181 ksi | At 1 mm/min; ISO 527-2 |
Borealis Bormed™ HF840MO Polypropylene Homopolymer for Medical Applications Bormed HF840MO is a polypropylene homopolymer intended for injection molding and is modified with an internal lubricant for products requiring a low surface friction (e.g. two-part syringes).Bormed .. |
|||
Tensile Modulus | 1.25 GPa | 181 ksi | 1mm/min; ISO 527-2 |
Borealis Daplen™ ED117AE Polypropylene TPO Compound Daplen™ ED117AE is a 10% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties and gives a good surfac.. |
|||
Tensile Modulus | 1.25 GPa | 181 ksi | ASTM-D790 |
Polyram RamLloy PVB101 ABS/NYLON alloy, Impact Modified Impact modified ABS/NYLON alloy for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Tensile Modulus | 1.25 GPa | 181 ksi | ISO 527-2 |
Total PPC 11712 Polypropylene, Heterophasic Copolymer ATOFINA Propylene 11712 is a nucleated controlled-rheology heterophasic copolymer. PPC 11712 is characterized by good stiffness and impact resistance as well as low shrinkage and low warpage. It h.. |
|||
Tensile Modulus | 1.25 GPa | 181 ksi | ISO 527-2 |
Total PPC 9612 Polypropylene, Heterophasic Copolymer, Injection Molding This product is a Total Ecosolutions grade.Polypropylene PPC 9612 has been developed specifically for the injection molding of crates and is characterized by a high Melt Flow index of 20 g/10 min. .. |
|||
Tensile Modulus | 1.25 GPa | 181 ksi | 1mm/min; ISO 527-2 |
Borealis RD360MO Polypropylene Random Copolymer, Transparent RD360MO is a specially modified highly-transparent polypropylene random copolymer with medium melt flow rate. This grade is designed for high-speed injection molding and contains nucleating and ant.. |
|||
Tensile Modulus | 1.25 GPa | 181 ksi | ISO 527-2 |
Total PPC 11750 Polypropylene, Heterophasic Copolymer, Injection Molding Polypropylene PPC 11750 is a nucleated and controlled-rheology heterophasic copolymer with very high Melt Flow index of 50 g/10 min.Polypropylene PPC 11750 is characterized by good impact resistance.. |
|||
Tensile Modulus | 1.25 GPa | 181 ksi | ISO 527-2 |
Total PPC 3650 Polypropylene, Heterophasic Copolymer, Injection Molding Polypropylene PPC 3650 is a heterophasic copolymer with a Melt Flow index of 2 g/10 min.Polypropylene PPC 3650 provides an excellent balance between toughness and flow, being particularly suitable i.. |
|||
Tensile Modulus | 1.25 GPa | 181 ksi | ISO 527-2 |
Total PPC 4640 Polypropylene, Heterophasic Copolymer ATOFINA Polypropylene PPC 4640 is a nucleated copolymer. PPC 4640 is characterized by good stiffness and impact resistance coupled with high creep resistance. |
|||
Tensile Modulus | 1.25 GPa | 181 ksi | Secant; ISO 527-2 |
ExxonMobil Exxtral™ CNU 012 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin designed for injection molded automotive applications. Availability: Africa & Middle East, Asia Pacific, Europe, South America and Nor.. |
|||
Tensile Modulus | 1.25 GPa | 181 ksi | Secant; ISO527-2/1 |
ExxonMobil PP7054L1 Polypropylene Impact Copolymer Product Description: A nucleated impact copolymer resin with medium flow. It is suitable for molding applications like consumer products, closures, containers, toys and rigid packaging applications.. |
|||
Tensile Modulus | 1.25 GPa | 181 ksi | Secant; ISO527-2/1 |
ExxonMobil PP7075L1 Polypropylene Impact Copolymer Product Description: A nucleated impact copolymer resin with high flow and antistatic properties. It is suitable for molding applications like disposable houseware, consumer products, toys and rigi.. |
|||
Tensile Modulus | 1.25 GPa | 181 ksi | |
BASF Novolen® 2300 L Polypropylene Injection molded parts.Data was collected by ISO methods and provided by BASF. |
|||
Tensile Modulus | 1.25 GPa | 181 ksi | |
BASF Novolen® 2309 L Polypropylene Cast film and thermoformed partsData was collected by ISO methods and provided by BASF. |
|||
Tensile Modulus | 1.25 GPa | 181 ksi | |
BASF Procom® X10S 773 Polypropylene Car bumpers and spoilers where good paintability is required.Data was collected by ISO methods and provided by BASF. |
|||
Tensile Modulus | 1.25 GPa | 181 ksi | 1mm/min; ISO 527 |
BASF Ultramid® 1003-2 NF2002 PA66 (Conditioned) Ultramid 1003-2 NF2002 is a general purpose, heat stabilized nylon 6/6. |
|||
Tensile Modulus | 1.25 - 1.40 GPa @Thickness 2.00 mm, Temperature 23.0 °C |
181 - 203 ksi @Thickness 0.0787 in, Temperature 73.4 °F |
Type IV, 1.0 mm/min; ASTM D638 |
Solvay Specialty Polymers Solef® 60512 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 60512 PVDF copolymer has high viscosity of the melt and it is a grade for offshore piping.Information provided by Solvay Specialty Polymers. |
|||
Tensile Modulus | 1.25 GPa | 181 ksi | |
BASF Novolen® 2440 K Polypropylene Data was collected by ISO methods and provided by BASF. |