Mechanical Properties Metric English Comments
Tensile Modulus 15.3 GPa
2220 ksi
ISO 527-1/-2
Lanxess Durethan® AKV 50 H2.0 901510 Nylon 66, 50% Glass Fiber
PA 66, injection molding grade, 50% glass fibers, good heat-ageing resistance
Tensile Modulus 15.3 GPa
2220 ksi
LATI Latilub 87/28-15T K/20 PC, 20% Carbon Fiber Reinforced, PTFE Filled
Self-lubricating product based on Polycarbonate (PC). PTFE. Carbon fiber. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria..
Tensile Modulus 15.3 GPa
2220 ksi
ISO 527-2
Solvay Specialty Polymers Amodel® DW-1140 Polyphthalamide (PPA), 40% Glass Fiber
Amodel® DW-1140 is a 40% glass-fiber-reinforced resin designed for high strength and stiffness and improved hydrolytic stability. This material has low moisture absorption and a low coefficient o..
Tensile Modulus 15.3 GPa
2220 ksi
ASTM D638
Plenco 5350 Phenolic, Granular, Injection Molded
PLENCO 05350 is a mineral and graphite filled phenolic molding compound, developed for seal applications. PLENCO 05350 offers excellent dimensional stability, lubricity, and low abrasion properties...
Tensile Modulus 15.3 GPa
2220 ksi
ASTM D638
Plenco 6015 Phenolic, Briquette, Transfer Molded
PLENCO 06015 is a glass and mineral filled phenolic molding compound offering improved mechanical strength, dimensional stability and excellent electrical properties. 06015 is available in black.Inf..