Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 1.37 GPa | 199 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP SP003 PA 12 LNP* LUBRICOMP* SP003 is a compound based on Nylon 12 resin containing 15% PTFE/Silicone. Added feature of this material is: Wear Resistant. |
|||
Tensile Modulus | 1.37 GPa | 199 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP SP003 PA 12 (Asia Pacific) LNP* Lubricomp* SP003 is a compound based on Nylon 12 resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated. |
|||
Tensile Modulus | 1.37 GPa | 199 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-LOY A3000T ABS (Asia Pacific) LNP* Stat-loy* A3000T is a compound based on Acrylonitrile Butadiene Styrene resin containing Anti-Static. Added features of this material include: Antistat. |
|||
Tensile Modulus | 1.37 GPa | 199 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Stat-loy A3000Z ABS LNP* Stat-loy* A3000Z is a compound based on Acrylonitrile Butadiene Styrene resin containing Anti-Static. Added features of this material include: Antistat.This data was supplied by SABIC-IP for t.. |
|||
Tensile Modulus | 1.37 GPa | 199 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Stat-loy A3000Z ABS (Asia Pacific) LNP* Stat-loy* A3000Z is a compound based on Acrylonitrile Butadiene Styrene resin containing Anti-Static. Added features of this material include: Antistat.This data was supplied by SABIC-IP for t.. |
|||
Tensile Modulus | 1.37 GPa | 199 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL PPX PPX7115 PPE+PP High modulus/impact/heat PPE+PP |
|||
Tensile Modulus | 1.37 GPa | 199 ksi | Secant; ISO 527-2 |
ExxonMobil Exxtral™ BMU 133 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin characterized by a good stiffness/toughness balance and designed for paintable automotive exterior applications.Availability: Europe .. |
|||
Tensile Modulus | 1.37 GPa | 199 ksi | Secant; ISO 527-2/50 |
ExxonMobil Exxtral™ BNU 011 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin characterized by a good stiffness/toughness balance and designed for injection molded automotive interior applications.Availability: A.. |
|||
Tensile Modulus | 1.37 GPa | 199 ksi | ISO527-2/1 |
ExxonMobil PP7555KNE2 Polypropylene Impact Copolymer Product Description: A high melt flow rate medium impact copolymer resin designed for thin wall injection molding requiring fast cycle time and low odor.Availability: Asia Pacific Features:Good Mol.. |