Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Styron CALIBREâ„¢ 2061-22 Polycarbonate Resin

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer Styron
Trade Name CALIBRE™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Styron CALIBREâ„¢ 2061-22 Polycarbonate Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Overview: CALIBREâ„¢ 2061-22 resin is suitable for steam and ethylene oxide sterilization required by the health care industry. CALIBRE 2061-22 provides exceptional clarity, heat resistance, impact strength, and processability, and has low contamination levels. CALIBRE 2061-22 resin has undergone biocompatibility testing based on ISO 10993 (Biological Evaluation of Medical Devices) and is suitable for use in approved medical applications. This product contains mold release. Main Characteristics:ISO 10993Applications:Medical applicationsInformation provided by Styron
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ISO 1183/A; ASTM D792
Water Absorption 0.32 %

@Temperature 23.0 °C
0.32 %

@Temperature 73.4 °F
Equilibrium, 50% RH; ISO 62; ASTM D570
0.15 %

@Temperature 23.0 °C,
Time 86400 sec
0.15 %

@Temperature 73.4 °F,
Time 24.0 hour
ISO 62; ASTM D570
Melt Flow 22 g/10 min

@Load 1.20 kg,
Temperature 300 °C
22 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238; ISO 1133
Mechanical Properties Metric English Comments
Hardness, Rockwell R 118
118
ASTM D785
Tensile Strength at Break 65.5 MPa
9500 psi
50 mm/min; ASTM D638
66.0 MPa
9570 psi
ISO 527-2/50
Tensile Strength, Yield 60.0 MPa
8700 psi
50 mm/min; ISO 527-2/50; ASTM D638
Elongation at Break 120 %
120 %
50 mm/min; ISO 527-2/50; ASTM D638
Tensile Modulus 2.34 GPa
339 ksi
50 mm/min; ISO 527-2/50; ASTM D638
Flexural Strength 96.5 MPa
14000 psi
Method I (3 point load), 2.0 mm/min; ISO 178; ASTM D790
Flexural Modulus 2.41 GPa
350 ksi
Method I (3 point load), 2.0 mm/min; ISO 178; ASTM D790
Izod Impact, Notched 7.50 J/cm

@Temperature 23.0 °C
14.1 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Izod Impact, Notched (ISO) 73.0 kJ/m²

@Temperature 23.0 °C
34.7 ft-lb/in²

@Temperature 73.4 °F
ISO 180/A
Dart Drop, Total Energy 72.3 J
53.3 ft-lb
3.39 m/sec; ASTM D3763
Abrasion 45
45
[%] Taber; ASTM D1044
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 68.0 µm/m-°C

@Temperature -40.0 - 82.0 °C
37.8 µin/in-°F

@Temperature -40.0 - 180 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 142 °C
288 °F
Annealed; ISO 75-2/B; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 126 °C
259 °F
Unannealed; ASTM D648; ISO 75-2/A
126 °C
259 °F
Annealed; ASTM D648; ISO 75-2/A
Vicat Softening Point 152 °C

@Load 5.10 kg
306 °F

@Load 11.2 lb
Rate A (50°C/h); ISO 306/B50; ASTM D1525
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
Optical Properties Metric English Comments
Refractive Index 1.586
1.586
ASTM D542; ISO 489
Haze 1.0 %
1.0 %
ASTM D1003
Transmission, Visible 89 %
89 %
ASTM D1003
Electrical Properties Metric English Comments
Volume Resistivity 2.00e+17 ohm-cm
2.00e+17 ohm-cm
ASTM D257
Dielectric Constant 3.0

@Frequency 60.0 Hz
3.0

@Frequency 60.0 Hz
ASTM D150
3.0

@Frequency 1.00e+6 Hz
3.0

@Frequency 1.00e+6 Hz
ASTM D150
Dielectric Strength 17.0 kV/mm
432 kV/in
ASTM D149
17.0 kV/mm
432 kV/in
IEC 60243-1
Dissipation Factor 0.0010

@Frequency 50.0 Hz
0.0010

@Frequency 50.0 Hz
ASTM D150
0.0020

@Frequency 1.00e+6 Hz
0.0020

@Frequency 1.00e+6 Hz
ASTM D150
Descriptive Properties Value Comments
Average Extent of Burring 3 cm
ASTM D635
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved