Tensile Modulus 7.75 GPa
1120 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics NORYL PX5558 PPE+PS
30% glass reinforced, high flow PPO.
Tensile Modulus 7.75 GPa
1120 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics NORYL EM7430 PPE+PS
30% glass reinforced, high flow PPO. Automotive. Energy management material.
Tensile Modulus 7.75 GPa
1120 ksi
ISO 527
Polyram Polytron P30N11 Polypropylene, 30% Long Fiber Glass
A chemically coupled 30% long fiber glass reinforced natural polypropylene, heat stabilized, for injection molding applications.Information provided by Polyram.
Tensile Modulus 7.75 GPa
1120 ksi
ISO 527
Polyram Polytron P30B07 Polypropylene, 30% Long Glass Fibers, UV Stabilized
A chemically coupled 30% long glass fibers reinforced black polypropylene, heat stabilized, UV stabilized for injection molding applications.Information provided by Polyram.
Tensile Modulus 7.75 GPa
1120 ksi
ASTM-D790
Polyram Polytron P30N01 Homopolymer Polypropylene, Chemically Coupled 30% Long Fiber
A CHEMICALLY COUPLED 30% LONG FIBER GLASS REINFORCED NATURAL POLYPROPYLENE HEAT STABILIZED FOR INJECTION MOLDING APPLICATION.Information provided by Polyram Ram On Ind.
Tensile Modulus 7.75 GPa

@Temperature -35.0 °C
1120 ksi

@Temperature -31.0 °F
Dynamic; ISO 11403-1 -2
DuPont Performance Polymers Crastin® LW9020 NC010 PBT+ASA  (Unverified Data**)
20% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9020 NC010 is a 20% glass fiber reinforced polybutylene terephthalate blend for injection molding. ..
Tensile Modulus 7.75 GPa
1120 ksi
Radici Radilon® A RV300R (cond.) Nylon 66
Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov..
Tensile Modulus 7.75 GPa
1120 ksi
ASTM-D790
Polyram Polytron P30B01 Homopolymer Polypropylene, Chemically Coupled 30% LGF
A chemically coupled 30% LGF reinforced black PP, heat stabilized for high temperature applications such as under the hood automotive parts.Information provided by Polyram Ram On Ind.
Tensile Modulus 7.75 GPa
1120 ksi
ASTM-D790
Polyram Polytron P30B11 Homopolymer Polypropylene, Chemically Coupled 30% LGF
A chemically coupled 30% LGF reinforced black PP, heat stabilized for injection molding applications.Information provided by Polyram Ram On Ind.