Material Notes:
A chemically coupled 30% long fiber glass reinforced natural polypropylene, heat stabilized, for injection molding applications.Information provided by Polyram.
Physical Properties Metric English Comments
Density 1.12 g/cc
0.0405 lb/in³
ISO 1183
Linear Mold Shrinkage 0.0017 cm/cm
0.0017 in/in
ISO 2577
Mechanical Properties Metric English Comments
Tensile Strength, Yield 110 MPa
16000 psi
ISO 527
Elongation at Break 2.6 %
2.6 %
ISO 527
Tensile Modulus 7.75 GPa
1120 ksi
ISO 527
Flexural Strength 160 MPa
23200 psi
ISO 178
Flexural Modulus 6.45 GPa
935 ksi
ISO 178
Izod Impact, Notched (ISO) 18.0 kJ/m²
8.57 ft-lb/in²
ISO 180
Charpy Impact Unnotched 6.00 J/cm²
28.6 ft-lb/in²
ISO 179
Charpy Impact, Notched 1.80 J/cm²
8.57 ft-lb/in²
ISO 179
Thermal Properties Metric English Comments
Melting Point 167 °C
333 °F
ISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 149 °C
300 °F
ISO 75
Flammability, UL94 HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in
Flame Spread 30 mm/min
1.2 in/min
FMVSS302
Glow Wire Test 750 °C
1380 °F
G.W.I.T.; IEC 60695