Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polyram Polytron P30B11 Homopolymer Polypropylene, Chemically Coupled 30% LGF

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 30% Glass Fiber Filler
Manufacturer Polyram
Trade Name Polytron
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyram Polytron P30B11 Homopolymer Polypropylene, Chemically Coupled 30% LGF.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A chemically coupled 30% LGF reinforced black PP, heat stabilized for injection molding applications.Information provided by Polyram Ram On Ind.
Physical Properties Metric English Comments
Density 1.06 g/cc
0.0383 lb/in³
ASTM-D792
Linear Mold Shrinkage 0.0017 cm/cm
0.0017 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Yield 100 MPa
14500 psi
ASTM-D638
Elongation at Break 2.6 %
2.6 %
ASTM-D638
Tensile Modulus 7.75 GPa
1120 ksi
ASTM-D790
Flexural Strength 150 MPa
21800 psi
ASTM-D790
Flexural Modulus 6.45 GPa
936 ksi
ASTM-D790
Izod Impact, Notched 1.80 J/cm

@Temperature 23.0 °C
3.37 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 149 °C
300 °F
ASTM-D648
Flammability, UL94 HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in
Flame Spread 13.3 mm/min
0.524 in/min
FMVSS302
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved