Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 21.0 MPa
3050 psi
ISO 527
Premix Thermoplastics PRE-ELEC® ESD 4400 Static Dissipative Thermoplastic Compound
PRE-ELEC® ESD 4400 is a static dissipative thermoplastic compound based on PE-LD. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD 4400 has been developed for ..
Film Tensile Strength at Break, TD 21.0 MPa
3050 psi
ASTM D882
NOVA Chemicals Sclair® 11L2B Octene LLDPE Film Resin  (discontinued **)
Film Properties. Features: Low gel, excellent seal characteristics, easy processability.Applications: Specialty lamination, co-extrusion of food and liquid packaging.Data provided by the manufactur..
Film Tensile Strength at Break, TD 21.0 MPa
3050 psi
ASTM D882
Huntsman Rexell® M3104 Blown Film Extrusion LLDPE  (discontinued **)
Linear-low medium density copolymer, cast film extrusion, FDA compliant.Features: Excellent combination of toughness, stiffness, and optics with good temperature resistance.Applications: Diaper film..
Film Tensile Strength at Break, TD 21.0 MPa
3050 psi
ASTM D882
Chevron Phillips 5036 LDPE High Clarity, Impact Film Resin  (discontinued **)
Resin Type: Homopolymer; for General Purpose PackagingCharacteristics: Excellent Clarity, Good Impact Strength, High Slip, No Antiblock, Low Coefficient of Friction, Excellent ProcessabilityApplicat..
Film Tensile Strength at Break, TD 21.0 MPa
3050 psi
ASTM D882
Eastman E6838-902F Polyethylene Film  (discontinued **)
Polyethylene E6838-902F natural contains slip and antiblock and is suggested for film applicationsApplications/UsesFood - contact applicationsEastman Chemical Company sold its polyethylene business ..
Film Tensile Strength at Break, TD 21.0 MPa
3050 psi
ASTM D882
Eastman E6838-899F Polyethylene  (discontinued **)
E6838-899F is a low density formulation with no slip or antiblock. It is suggested for film applications requiring high clarity, good tear and impact strength, a wide heat-sealing range, and good pr..
Film Tensile Strength at Break, TD 21.0 MPa
3050 psi
ASTM D882
Eastman E6838-964F Polyethylene  (discontinued **)
E6838-964F is a low density formulation with medium slip and medium antiblock. It is suggested for film applications that require a good balance of physical and optical properties.List of Applicati..
Film Tensile Strength at Break, TD 21.0 MPa
3050 psi
ASTM D882
ExxonMobil Escorene® LD-140 LDPE Industrial Film resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A fractional melt index homopolymer resin for production of film with very good toughness.Applications: Heavy duty bags. Data for film properties b..
Film Tensile Strength at Break, TD 21.0 MPa
3050 psi
ASTM D882
Huntsman PE 1008 Film Extrusion Polyethylene  (discontinued **)
Homopolymer, and FDA compliant.Features: Superior strength, good machinability, and heat seal characteristics.Applications: Film extrusion: industrial packaging, frozen food, produce bags, shrink, a..
Film Tensile Strength at Break, TD 21.0 MPa
3050 psi
ASTM D882
Huntsman PE1031 Film Extrusion Polyethylene  (discontinued **)
Homopolymer, and FDA compliant.Features: Superior strength, good machinability, and heat seal characteristics.Applications: Film extrusion: clarity packaging, frozen food, produce bags, shrink, bund..
Film Tensile Strength at Break, TD 21.0 MPa
3050 psi
ASTM D882
Chevron Phillips HiD® 9606 HDPE Blown Film and Sheet  (discontinued **)
Resin Type: ASTM D 4976 Classification: PE 235, A 54502Applications:General Purpose Films and Sheet, Coextruded Film Structures, Deli and Tissue Films, Sheet Thermoforming Applications with Good Str..
Film Tensile Strength at Break, TD 21.0 MPa
3050 psi
ASTM D882
ExxonMobil Escorene® LD-141 EVA Shrink Film Resin, FMI  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A fractional melt index, 2.0% vinyl acetate copolymer film resin with very good toughness and shrink properties. The low melt index gives excellent..
Film Tensile Strength at Break, TD 21.0 MPa
3050 psi
ASTM D882
ExxonMobil Escorene® LD-318 EVA Film Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A 9.0% vinyl acetate copolymer film resin. Film made from LD-318 exhibits superior impact strength and heat sealability.Applications: Primal meat b..
Film Tensile Strength at Break, TD 21.0 MPa
3050 psi
ASTM D882
ExxonMobil Escorene® LD-319 EVA Film Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A 9.0% vinyl acetate copolymer film resin. Film made from LD-319 exhibits superior impact strength and heat sealability.Applications: Primal meat b..
Film Tensile Strength at Break, TD 21.0 MPa
3050 psi
ASTM D882
ExxonMobil Escorene® LD-334 EVA Film Resin, Clarity, High Impact  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A 4.2% vinyl acetate copolymer, clarity film resin. The low melt index and comonomer context of this resin help produce films with superior impact ..
Film Tensile Strength at Break, TD 21.0 MPa
3050 psi
ASTM D882
Petroquimica Triunfo Trithene® TX 8024 LDPE - High Clarity Film
The Trithene TX 8024 resin is a low-density polyethylene (LDPE) with high molecular weight and distribution narrow, designed to obtain films with very high clarity and excellent processability. This..
Film Tensile Strength at Break, TD 21.0 MPa
3050 psi
ASTM D882
Metabolix M-veraâ„¢ B5008 Film Grade Compostable Bioplastic
B5008 is a compostable film product with 30% biobased carbon content that is ideal for compost bags and can liners used for organic waste diversion and for shopping and retail bags.Features:Meets re..
Film Tensile Strength at Break, TD 21.0 MPa
3050 psi
ISO R527-1
Iran Petrochemical (PCC) 2101TN47 Low Density Polyethylene
LDPE 2101TN47 Shrink FilmThis grade enables high speed production of film without blocking.Information provided by Iran Petrochemical Commercial Co.
Film Tensile Strength at Break, TD 21.0 MPa
3050 psi
ASTM-D882
Braskem TS7010 LDPE Blown Film Extrusion Polyethylene
TS7010 is a low-density polyethylene (LDPE) that presents excellent processability and good mechanical properties. The incorporated additives package warrants a low coefficient of friction (COF) all..
Film Tensile Strength at Break, TD 21.0 MPa
3050 psi
ASTM-D882
Braskem TX7012 LDPE Blown Film Extrusion Polyethylene
TX7012 is a low-density polyethylene (LDPE) with medium molecular weight and good processability in traditional extruders with good mechanical properties and productivity, ensuring uniform thickness..
Film Tensile Strength at Break, TD 21.0 MPa
3050 psi
ASTM D882
Huntsman PE1061 Film Extrusion Polyethylene  (discontinued **)
Homopolymer and FDA compliant.Features: Exceptional strength, good machinability and heat seal characteristics.Applications: Film extrusion: high clarity packaging, frozen food, produce bags, shrink..
Film Tensile Strength at Break, TD 21.0 - 48.0 MPa
3050 - 6960 psi
Average value: 38.8 MPa Grade Count:34
Overview of materials for Linear Low Density Polyethylene (LLDPE)/Octene, Film
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE)/Octene, Film". Each property range of values reported is minimum..
Film Tensile Strength at Break, TD 21.0 MPa
3050 psi
ASTM D882
Huntsman PE 1253 EVA Film Extrusion  (discontinued **)
2.5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, good heat seal characteristics.Applications: Film extrusion: general purpose packaging where to..
Film Tensile Strength at Break, TD 21.0 MPa
3050 psi
ASTM D882
NOVA Chemicals Sclair® 11L4B Octene LLDPE Film Resin  (discontinued **)
Film Properties. Features: Low gel, excellent seal characteristics.Applications: Specialty lamination, co-extrusion of food and liquid packaging.Data provided by the manufacturer.
Film Tensile Strength at Break, TD 21.0 MPa
3050 psi
ASTM D882
Huntsman PE1353 EVA Film Extrusion  (discontinued **)