Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 82.7 MPa | 12000 psi | ASTM D790 |
Ensinger ENSITEP® PBT Polybutylene Terephthalate - Extruded Products
(discontinued **) ENSITEP BT is an unreinforced thermoplastic polyester derived from polybutylene terephthalate. Its excellent wear and impact resistance, low coefficient of friction, high flexural modulus, and supe.. |
|||
Flexural Yield Strength | 82.7 MPa | 12000 psi | ASTM D790 |
Albis Plastics PC/PET 361E Unfilled
(discontinued **) Amorphous Polycarbonate /Polyethylene Terephthalate Blend (PC/PET)Characteristics: High Strength, Rigidity and Creep Resistance. Good Chemical ResistanceApplications: Pump Components, Industrial and.. |
|||
Flexural Yield Strength | 82.7 - 131 MPa | 12000 - 19000 psi | Average value: 93.5 MPa Grade Count:35 |
Overview of materials for Polycarbonate, Optical Grade This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Optical Grade". Each property range of values reported is minimum and maximum values of a.. |
|||
Flexural Yield Strength | 82.7 - 245 MPa | 12000 - 35500 psi | Average value: 126 MPa Grade Count:14 |
Overview of materials for Nylon 66, Mineral Filled, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Mineral Filled, Impact Grade". Each property range of values reported is minimum and maximum v.. |
|||
Flexural Yield Strength | 82.7 - 100 MPa | 12000 - 14500 psi | Average value: 92.2 MPa Grade Count:4 |
Overview of materials for Nylon 11 with 10% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with 10% Glass Fiber Filler". Specific grades with glass content between 5% and 14% are includ.. |
|||
Flexural Yield Strength | 82.7 MPa | 12000 psi | ASTM D790 |
Global GP-150 High Impact Polystyrene High flowGood stiffnessApplications:AppliancesElectrical/Electronic applicationsHousehold goodsFood packagingToys |
|||
Flexural Yield Strength | 82.7 MPa | 12000 psi | ASTM D790 |
Techmer ES Elastoblend® PA6/6 IM 408 L Nylon 66 Availability: North AmericaForms: PelletsAdditive: Lubricant and Impact ModifierFeatures: Lubricant and Impact ModifiedProcessing Method: Injection MoldingInformation provided by TP Composites, Inc... |
|||
Flexural Yield Strength | 82.7 MPa | 12000 psi | ASTM D790 |
Techmer ES Elastoblend® PA6/6 IM5 BK Nylon 66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubricant and Impact ModifiedProcessing Method: Injection MoldingInformati.. |
|||
Flexural Yield Strength | 82.7 MPa | 12000 psi | ASTM D790 |
Techmer ES HiFill FR® PC IM FR Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Flame Retardant and Impact ModifiedProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Flexural Yield Strength | 82.7 MPa | 12000 psi | ASTM D790 |
Star Plastics PC/ABSQX7004 Molding Grade PC/ABS Information provided by Star Plastics, Inc. |
|||
Flexural Yield Strength | 82.7 MPa | 12000 psi | ASTM D790 |
Star Plastics PC/PBT7820 Molding Grade PC/PBT Information provided by Star Plastics, Inc. |
|||
Flexural Yield Strength | 82.7 MPa | 12000 psi | ASTM D790 |
Star Plastics PC/PBTQX7008 Molding Grade PC/PBT Information provided by Star Plastics, Inc. |
|||
Flexural Yield Strength | 82.7 MPa | 12000 psi | ASTM D790 |
Techmer ES HiFill® POM HO UV Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: HomopolymerInformation provided by TP Composites, Inc. |
|||
Flexural Yield Strength | 82.7 MPa | 12000 psi | ASTM D790 |
Techmer ES Plastiblend® PC/ABS FR 6206 Availability: North AmericaForms: PelletsFeatures: Flame RetardantInformation provided by TP Composites, Inc. |
|||
Flexural Yield Strength | 82.7 MPa | 12000 psi | ASTM D790 |
Techmer ES Plastiblend® PC/ABS FR 6206 UV Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: Flame RetardantInformation provided by TP Composites, Inc. |
|||
Flexural Yield Strength | 82.7 MPa | 12000 psi | ASTM D790 |
Techmer ES Statiblend® PC/ABS 830 SS7 BK with Stainless Steel Fiber Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 7% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Flexural Yield Strength | 82.7 MPa | 12000 psi | ASTM D790 |
Techmer ES Elastoblend® PA6/6 IM 408 HS L Nylon 66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubricant and Impact ModifiedProcessing Method: Injection MoldingInformati.. |
|||
Flexural Yield Strength | 82.7 MPa | 12000 psi | ASTM D790 |
PlastxWorld CEVIAN® DR210 PC Alloy High impact, good flowability and heat resistant.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Flexural Yield Strength | 82.7 MPa | 12000 psi | ASTM D790 |
Clariant Renol BR7008 Polycarbonate/Polyester Alloy Data provided by Clariant Masterbatches |
|||
Flexural Yield Strength | 82.7 MPa | 12000 psi | ASTM D790 |
Clariant Renol PA123 Nylon 66, Impact Modified, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Flexural Yield Strength | 82.7 MPa | 12000 psi | ASTM D790 |
Clariant Renol PA2SP0017 Nylon 6, Impact Modified Data provided by Clariant Masterbatches |
|||
Flexural Yield Strength | 82.7 MPa | 12000 psi | ASTM D790 |
Clariant Renol PA121 Nylon 66, Impact Modified Data provided by Clariant Masterbatches |
|||
Flexural Yield Strength | 82.7 - 134 MPa | 12000 - 19500 psi | Average value: 102 MPa Grade Count:7 |
Overview of materials for PC/ABS + Stainless Steel This property data is a summary of similar materials in the MatWeb database for the category "PC/ABS + Stainless Steel". Each property range of values reported is minimum and maximum values of appro.. |
|||
Flexural Yield Strength | 82.7 - 186 MPa | 12000 - 27000 psi | Average value: 121 MPa Grade Count:11 |
Overview of materials for Acrylic/Polycarbonate Alloy, Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Acrylic/Polycarbonate Alloy, Glass Fiber Filler". Each property range of values reported is minimum and .. |
|||
Flexural Yield Strength | 82.7 - 276 MPa | 12000 - 40000 psi | Average value: 184 MPa Grade Count:3 |
Overview of materials for Polyphenylene Sulfide (PPS), NCG Fiber This property data is a summary of similar materials in the MatWeb database for the category "PPS + NGG". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |
|||
Flexural Yield Strength | 82.7 MPa | 12000 psi | ASTM D790 |
Styron PULSE™ EXT 100 PC/ABS Engineering Resin Overview: PULSE EXT 100 engineering resin has been designed to provide excellent processability, high heat resistance, and high impact strength at both room and low temperatures. PULSE EXT 100 engin.. |