Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 70.0 - 186 MPa | 10200 - 27000 psi | Average value: 123 MPa Grade Count:31 |
Overview of materials for Acetal Copolymer, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% ar.. |
|||
Flexural Yield Strength | 138 - 186 MPa | 20000 - 27000 psi | Average value: 165 MPa Grade Count:8 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 30% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 30% Carbon Fiber Filled". Specific grades with carbon fiber conte.. |
|||
Flexural Yield Strength | 86.0 - 186 MPa | 12500 - 27000 psi | Average value: 95.9 MPa Grade Count:14 |
Overview of materials for Polycarbonate, High Heat This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, High Heat". Each property range of values reported is minimum and maximum values of appro.. |
|||
Flexural Yield Strength | 82.7 - 186 MPa | 12000 - 27000 psi | Average value: 111 MPa Grade Count:115 |
Overview of materials for Polycarbonate, 10% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 10% Glass Filled". Specific grades with glass content between 5% and 14% are included. Ea.. |
|||
Flexural Yield Strength | 17.2 - 186 MPa | 2500 - 27000 psi | Average value: 71.9 MPa Grade Count:52 |
Overview of materials for High Density Polyethylene (HDPE), Glass fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Glass fiber Filled". Each property range of values reported is minimum.. |
|||
Flexural Yield Strength | 36.5 - 186 MPa | 5300 - 27000 psi | Average value: 77.2 MPa Grade Count:99 |
Overview of materials for Acetal Copolymer, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, PTFE Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Flexural Yield Strength | 82.7 - 186 MPa | 12000 - 27000 psi | Average value: 121 MPa Grade Count:11 |
Overview of materials for Acrylic/Polycarbonate Alloy, Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Acrylic/Polycarbonate Alloy, Glass Fiber Filler". Each property range of values reported is minimum and .. |
|||
Flexural Yield Strength | 55.0 - 186 MPa | 7980 - 27000 psi | Average value: 101 MPa Grade Count:26 |
Overview of materials for Polybutylene Terephthalate (PBT), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Mineral Filled". Each property range of values reported is minimum and.. |
|||
Flexural Yield Strength | 31.0 - 186 MPa | 4500 - 27000 psi | Average value: 75.4 MPa Grade Count:18 |
Overview of materials for Polypropylene, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Carbon Fiber 10%". Each property range of values reported is minimum and maximum values o.. |