Mechanical Properties Metric English Comments
Flexural Yield Strength 85.0 - 276 MPa
12300 - 40000 psi
Average value: 153 MPa Grade Count:12
Overview of materials for Polyetheretherketone, PEEK, Aramid Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, PEEK, Aramid Fiber Filled". Each property range of values reported is minimum and ..
Flexural Yield Strength 39.0 - 276 MPa
5660 - 40000 psi
Average value: 101 MPa Grade Count:94
Overview of materials for Nylon 66, Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum ..
Flexural Yield Strength 186 - 276 MPa
27000 - 40000 psi
Average value: 225 MPa Grade Count:7
Overview of materials for Nylon 11 + Carbon Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 + Carbon Fiber". Each property range of values reported is minimum and maximum values of approp..
Flexural Yield Strength 28.0 - 276 MPa
4060 - 40000 psi
Average value: 92.9 MPa Grade Count:32
Overview of materials for Nylon 6, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Extruded". Each property range of values reported is minimum and maximum values of appropriate ..
Flexural Yield Strength 82.7 - 276 MPa
12000 - 40000 psi
Average value: 184 MPa Grade Count:3
Overview of materials for Polyphenylene Sulfide (PPS), NCG Fiber
This property data is a summary of similar materials in the MatWeb database for the category "PPS + NGG". Each property range of values reported is minimum and maximum values of appropriate MatWeb e..
Flexural Yield Strength 60.0 - 276 MPa

@Temperature -40.0 - 150 °C
8700 - 40000 psi

@Temperature -40.0 - 302 °F
Average value: 150 MPa Grade Count:3
Overview of materials for Polyethylene Terephthalate (PET), 30% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 30% Glass Reinforced". Specific grades with glass content between 25% ..