Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 69.0 - 89.8 MPa | 10000 - 13000 psi | Average value: 78.9 MPa Grade Count:12 |
Overview of materials for Phenolic, Novolac, Heat Resistant Grade, Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Heat Resistant Grade, Filled". Each property range of values reported is minimum and .. |
|||
Flexural Yield Strength | 51.7 - 89.6 MPa | 7500 - 13000 psi | Average value: 77.0 MPa Grade Count:3 |
Overview of materials for Nylon 11, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11, Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Flexural Yield Strength | 62.1 - 89.6 MPa | 9000 - 13000 psi | Average value: 77.9 MPa Grade Count:23 |
Overview of materials for Acetal Homopolymer, PTFE-Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, PTFE-Filled". Each property range of values reported is minimum and maximum values o.. |
|||
Flexural Yield Strength | 8.96 - 89.6 MPa | 1300 - 13000 psi | Average value: 68.6 MPa Grade Count:41 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber Filled". Each property range of values repo.. |