Mechanical Properties Metric English Comments
Flexural Yield Strength 9.00 - 352 MPa

@Temperature -40.0 - 200 °C
1310 - 51100 psi

@Temperature -40.0 - 392 °F
Average value: 119 MPa Grade Count:22
Overview of materials for Polyphthalamide (PPA)
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide". Each property range of values reported is minimum and maximum values of appropriate Ma..
Flexural Yield Strength 110 - 352 MPa
16000 - 51100 psi
Average value: 253 MPa Grade Count:152
Overview of materials for Nylon 6, 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. E..
Flexural Yield Strength 261 - 352 MPa

@Temperature -40.0 - 60.0 °C
37900 - 51100 psi

@Temperature -40.0 - 140 °F
Average value: 154 MPa Grade Count:1
Overview of materials for Polyphthalamide (PPA), Glass Fiber 40%
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Glass Fiber 40%". Specific grades with glass content between 35% and 44% are included. ..